Share
Results 1 to 13 of 13

Thread: Where to buy magnesium tig filler rod???

  1. #1

    Default Where to buy magnesium tig filler rod???

    I have a friend with a couple short magnesium screed boards (for concrete). I was wanting to cut them true and weld together. I just need a few pieces of filler rod. Does it need to be an special mag filler??? Maybe if someone has a few they want to part with.

    Any other tips on welding Magnesium??? Don't see much on the forums about it. Thinking it is pretty close to welding Aluminum.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  2. #2
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Interesting... how is it joined now? There is a WT&T.com article about it, but it seems to be more directed toward repairs on castings, rather than joining magnesium pieces.
    http://www.weldingtipsandtricks.com/...magnesium.html

    There's also a Youtube posting from WT&T, which I can't view at this moment, and an article at Lincoln:
    http://www.lincolnelectric.com/en-us...magnesium.aspx
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  3. #3
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Brian
    I have Magnesium welding rod alloy AZ61A I have used to weld magnesium motorcycle racing wheels that have been damaged and it work very well. It is similar to welding aluminum I used the same 100% argon flow 10 to 12 LPM AC balance from 30% to 45% AC Frequency was from 120hz and up to 200hz on my 250EX. Yes you have to get the welding surface clean and the rod clean, the rods oxidize very easily sitting around they turn black. When welding magnesium the weld has a different color to it then when welding aluminum. Now getting the welding rod I had to by the minimum amount and that was about 50 rods they are light you get a lot per pound. It probably cost more for me to send you some rods then it will cost for you to buy them Canada / USA boarder line. Question are the screeds electric or air ones and can you take off the vibrators and move them?
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  4. #4

    Default

    Quote Originally Posted by DaveO View Post
    Interesting... how is it joined now?
    They are not joined or broken. They are 2 short screeds that I want to make longer. They are kind of pricey and shipping is a big killer for a 12' length. Since these are freebies, I thought wonder if I could stick them together.

    Quote Originally Posted by Kempy View Post
    Brian
    I have Magnesium welding rod alloy AZ61A
    Will have to do some searching. I have only found a couple places on ebay selling the filler and it was quite expensive. Will Do a better search with the alloy number.

    Question are the screeds electric or air ones and can you take off the vibrators and move them?
    These are just simple hand screeds... Will show you a link to give you an idea. Looks more like a load bar for a semi truck.

    Well the ones I got are not this pretty anymore but this will give you an idea.

    http://www.marshalltown.com/productD...x?prodID=14733
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  5. #5

    Default

    There you go... Airgas has a 3 pound tube for $600... Ah I don't think so...
    http://www.airgas.com/browse/product...uct=haraz61t30

    Kempy... What did yours cost you???
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  6. #6
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Brian
    You could just rivet a aluminum plates inside with counter sunk rivets or c/s screws, good luck. I could mail you some in a poster tube if you can't find any you can PM me. I paid $110.00 for 1lbs many, many years ago
    Last edited by Kempy; 07-17-2013 at 02:00 AM. Reason: missed a part
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  7. #7
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Here is a pretty good breakdown of the various filler alloys.

    http://www.keytometals.com/Article35.htm

    Not exactly what you want, but diluted into the base metal, this might work for you and it's cheap enough to at least give it a shot.

    http://www.ebay.com/itm/111100559996

    http://www.ebay.com/itm/120830637078
    Last edited by Rambozo; 07-17-2013 at 03:10 AM.
    Long arc, short arc, heliarc and in-the-dark!

  8. #8

    Default

    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  9. #9
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    I've only welded a little Mag for practice (I was bored at work one day-lol), and I believe I used the AZ-92A filler rod that sportbike posted above. I don't know the exact requirements or sizing of the parts you plan to weld, or what type the mag you have is, but I welded on a few VW engine cases that were AS-21 and AS-41 with almost zero difficulty. I did have to preheat and post heat my parts when finished due to their size and the size of the cracked areas I was welding up, and I quickly realized that I needed to clean the beads after each pass. I was able to get a minimal amount of filler rod for free from a buddy that did a lot of mag repair on motorcycle applications.

    From what I hear, some motorcycle shops do a lot of repair work on cases and they may be able to sell you just a small amount of the rod you need. I was afraid of starting some major magnesium fire and burning down the entire world (after hearing horror stories and how mag can't be welded safely), but my worries went away once I realized idiots had fed me incorrect info.

    I know from my teen years that heavy chunks don't just start burning immediately (even when thrown in a bonfire), but the dust and chips themselves are VERY dangerous to work around!
    Last edited by youngnstudly; 07-18-2013 at 06:24 AM.
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  10. #10
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    I had a small fire once was grinding down some magnesium on a belt sander and forgot and did some steel later up in smoke glade I did not grind a lot of magnesium.
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  11. #11
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    Quote Originally Posted by Kempy View Post
    I had a small fire once was grinding down some magnesium on a belt sander and forgot and did some steel later up in smoke glade I did not grind a lot of magnesium.
    It makes total sense that would happen, but I don't think that changing the belt would have dawned on me until after the fact! My friend got burned pretty bad after using a grinding bit in a die grinder to clearance a VW bellhousing. He said he was grinding away, the shavings started to pile up a little, and all of the sudden he accidently nicked one of the transmission mount (steel) bolts with the sanding drum at high RPM and BOOM! Happened right in his face as he kneeled down inside the engine compartment, but he was smart enough to wear a face shield at least, which took most of the heat. Burned his neck a little and the hair on his arms though. One little spark is all it takes.
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  12. #12
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    If you have a good, sharp chop saw with carbide teeth, maybe you could thinly slice off one end and use it as needed for mag filler?

    Also, if you made two clean-cut ends maybe they could be joined together autogenuously. I'm not sure how well that works with magnesium myself... But if you're out for a learning project, might as well give it a try and find out! However, having the thin slice available to use as filler could be very desirable it it turns out the autogenous mag welding isn't working very well (e.g., hot cracking issues like some aluminum alloys are known for).
    '13 Everlast 255EXT
    '07 Everlast Super200P

  13. #13

    Default

    Kempy, thanks for the info... I know it has been a while. We all know how back burner projects get. Looking to use the screed boards soon and thought it was time to work on them. Well they sure were dirty. A wire brush would not come close to cleaning them. I took a D/A sander with a 220 grit and cleaned the ends up. Took a little while even with that.

    I bought some AZ61 off Ebay. I waited a while to get a fair deal. The screed boards are about 2" x 4". You sure need to put some quick tack welds on them. They walk out of alignment fast from the heat. I sure don't keep up with TIG welding. Kind of lose my touch between jobs. Even though, they TIGed up really nice. Welded close to Aluminum. Didn't need a whole lot of heat. But the heat sure did radiate down the tubes fast.

    The 200DX is a nice machine. I think it is close to 2 years old and it has seen its fair share of projects. I am happy with it so far.

    Another learning experience.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

Similar Threads

  1. New to welding. Which filler rod?
    By Xman4u in forum General Welding Questions
    Replies: 2
    Last Post: 01-16-2015, 11:43 AM
  2. Neat video about welding and identifying magnesium
    By sportbike in forum TIG Welding (GTAW/GTAW-P)
    Replies: 0
    Last Post: 09-27-2013, 12:33 AM
  3. where to purchase magnesium tig rod AZ101??
    By mogo in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 10-07-2012, 12:18 PM
  4. Using MIG wire for TIG filler.
    By blasphemy000 in forum General Welder Questions
    Replies: 6
    Last Post: 10-11-2011, 01:17 AM
  5. TIG Filler
    By bigjoeinkg in forum TIG Welding (GTAW/GTAW-P)
    Replies: 13
    Last Post: 07-18-2011, 09:50 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •