    Default First 'project' ........ shortening a "hand truck"

    OK, only posting this because it's my VERY first MIG welding project. For reasons that will remain unwritten I needed to shorten a 'hand truck' by about 6". The 'hand truck' was made from ~1" thinwall steel tubing and I set the MIG at 17.5v and ~220 in/min.

    Started by cutting out ~6" from the middle section and then welding in a short 3/8" rebar for reinforcement:
    Click image for larger version. 

Name:	IMG_0625.jpg 
Views:	1043 
Size:	139.0 KB 
ID:	10233

    I then tacked the upper section of the hand truck frame/tubes to the rebar and lower tubes of the hand truck:
    Click image for larger version. 

Name:	IMG_0627.jpg 
Views:	1797 
Size:	132.5 KB 
ID:	10234

    Final welding and a 'generous' amount of grinding yielded a 'just fair' review from yours truly. No need to post those ugly pics!

    In hindsight I think the big shop fan blowing on me (~95 deg in the shop today) probably didn't help with the shielding gas. I'm still struggling a bit to not get 'mega lumps' that need serious grinder attention. Need to figure out how to lower the wire speed (to minimize the lumps) and still get enough amps to melt the base metal. ??? Any insight on that issue would be appreciated.

    cheers all
    JohnG
    imig 200
    PowerTig 210 EXT

  2. #2
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    I like the slits for added strength instead of just a butt joint. Seeing that popped an idea into my head, instead of rebar for reinforcement, maybe cut the removed section lengthwise (with a big fat kerf) and squeeze it inside as a sleeve. Slots front and back to weld to/through would make it extra stout.

    Sorry I don't have any welding knowlege to share, I'm still at the same place you are when it comes to MIG.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  3. #3

    Default

    Quote Originally Posted by redbeard View Post
    I like the slits for added strength instead of just a butt joint. Seeing that popped an idea into my head, instead of rebar for reinforcement, maybe cut the removed section lengthwise (with a big fat kerf) and squeeze it inside as a sleeve. Slots front and back to weld to/through would make it extra stout.

    Sorry I don't have any welding knowlege to share, I'm still at the same place you are when it comes to MIG.
    That's an interesting option on the bracing. Probably would have been a little easier to weld because the rebar was WAY thicker than the tubing.
    imig 200
    PowerTig 210 EXT

Similar Threads

  1. Project "Get Bent"
    By dzljon in forum Hobyist Projects
    Replies: 3
    Last Post: 03-05-2015, 01:57 AM
  2. First "real" TIG welding project coming up.
    By 225 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 12-27-2012, 07:48 PM
  3. Project From EmptyNester - Belt "guide" for hovercraft
    By EmptyNester in forum Off Road Fabrication
    Replies: 5
    Last Post: 10-10-2012, 04:01 AM
  4. Project 10 from d3javoodoo " Another Work in Progress"
    By Legacyartist247 in forum Metal Art
    Replies: 15
    Last Post: 07-30-2011, 07:14 AM
  5. Replies: 0
    Last Post: 06-09-2011, 06:33 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •