    Default Removing a broken bolt - steering box

    To give credit where due, I attempted (and succeeded) with this due to watching this Welding Tips and Tricks Video:
    http://www.weldingtipsandtricks.com/...oken-bolt.html

    I've got a 67 Cutlass Supreme Convertible and am spiffing up the engine compartment. I decided to take off the steering box. It's bolted to the frame with 3 bolts. 2 bolts came out whole and 1 didn't.

    Starting Point:
    Click image for larger version. 

Name:	steering_box_01.jpg 
Views:	897 
Size:	103.8 KB 
ID:	10219

    After removal.
    Click image for larger version. 

Name:	steering_box_02.jpg 
Views:	914 
Size:	80.5 KB 
ID:	10220

    There's the 3 bolts - 1 good, 1 partially rusted and one in pieces.
    Click image for larger version. 

Name:	steering_box_03.jpg 
Views:	901 
Size:	99.9 KB 
ID:	10221

    What's left in the steering box.
    Click image for larger version. 

Name:	steering_box_04.jpg 
Views:	916 
Size:	95.0 KB 
ID:	10222

    Putting on a nut with a washer to weld to the bolt.
    Click image for larger version. 

Name:	steering_box_05.jpg 
Views:	942 
Size:	122.7 KB 
ID:	10223

    Putting a nut on the other side in hopes that I could put a wrench on both sides.
    Click image for larger version. 

Name:	steering_box_06.jpg 
Views:	962 
Size:	97.0 KB 
ID:	10224

    After nuts are welded on both sides.
    Click image for larger version. 

Name:	steering_box_07.jpg 
Views:	916 
Size:	60.2 KB 
ID:	10225

    One snapped off.
    Click image for larger version. 

Name:	steering_box_08.jpg 
Views:	913 
Size:	88.8 KB 
ID:	10226

    Weld another nut on.
    Click image for larger version. 

Name:	steering_box_09.jpg 
Views:	877 
Size:	99.8 KB 
ID:	10227

    Yay, the nut on the left is turning!
    Click image for larger version. 

Name:	steering_box_10.jpg 
Views:	935 
Size:	94.3 KB 
ID:	10228
    Sean M
    Illinois
    I-Tig-200 (March 2012)
    Harbor Freight 90 Amp Flux core Mig
    (Sold this one but I might have picked up some bad habits -->) Harbor Freight 130 Amp lift-start Tig (the red one)

  2. #2

    Default

    And here's the end, with the bolt removed! I used a cut off disk in a dremmel to cut the bolt with the nut on the right.
    Click image for larger version. 

Name:	steering_box_11.jpg 
Views:	768 
Size:	102.8 KB 
ID:	10229
    Sean M
    Illinois
    I-Tig-200 (March 2012)
    Harbor Freight 90 Amp Flux core Mig
    (Sold this one but I might have picked up some bad habits -->) Harbor Freight 130 Amp lift-start Tig (the red one)

  3. #3

    Default

    Cool. Nice job. Jody is absolutely right. With the right TIG welder you can put a nice precise arc where you want. Pretty handy stuff. Thanks for posting the pictures!

  4. Default

    Very nice.

  5. #5

    Default

    putting a wrench on both sides is not too bad of an idea... too bad my broken bolts do not stick out on both sides 99.9% of the time
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

Similar Threads

  1. Removing the Ram Slop from a Harbor Freight 20 Ton Press
    By fyidiy in forum Other Custom Fabrications
    Replies: 18
    Last Post: 08-11-2017, 02:50 PM
  2. Steering 14 Bolt
    By GFab70 in forum Off Road Fabrication
    Replies: 0
    Last Post: 12-04-2015, 03:50 PM
  3. Removing Mill Scale from Hot Rolled Steel?
    By Spike in forum General Welding Questions
    Replies: 24
    Last Post: 02-20-2013, 01:49 AM
  4. luvin my Steering wheel
    By azlo in forum On Road Fabrication
    Replies: 5
    Last Post: 12-27-2012, 03:00 AM
  5. Removing the MIG torch WP-18 shield nozzle
    By everlastsupport in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 0
    Last Post: 07-26-2009, 03:24 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •