    OK, finally time to make the trek to the LWS and get going with the MIG. Got a list going with a few questions.

    Mostly will be welding not-very-clean steel between 1/8 and 1/2. Got a couple spools of wire already, 1lb ER70s6 .023 and part of an ancient spool of Verti-Cor70 dual-shield .035.

    And for the shopping list:

    Tips
    Diffusers
    Gas, the Verticor calls for 75/25, but I was actually leaning towards 80/20 for a better shot at spray transfer. Opinions needed.
    33lb ER70S6 for the go-to spool, I'm thinking .035.
    1lb Al, 4043 I presume?
    Hardfacing wire - abrasion resistant, any recommendations? Reasonably priced sources?
    MIG pliers, only $7 at HF, what the heck.
    Wire cleaning pads.
    Regulator

    Am I forgetting anything? Getting something I shouldn't be?
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Might as well add a pound of 5356 alum wire. Some drives do a lot better with that.
    Nozzle gel or spray.
    Mig gloves (depending on what you have now).

    All I can think of at the moment, but I'm sure I'm overlooking something.
    You already have pure argon for the alum, right?
    Long arc, short arc, heliarc and in-the-dark!

  3. #3
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    I tried 98% Argon/2% O2 for Spray Arc Transfer on steel it worked OK but with a little adjustment I got 75% Argon 25% co2 to work just fine, 80% Argon 20% Co2 I could not find any different for the price. I set the MTS250S to SYN Mig 24.0V 200A SYN to Steel and wire to .035 wire was S-6. And welded .375 plate to 1.5 X 1.5 bar. Good grinder is nice with different disc hard and soft.
    Click image for larger version. 

Name:	spray weld .035.jpg 
Views:	483 
Size:	129.7 KB 
ID:	10132
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  4. #4

    Default

    if its not too late maybe a roll of wire for stainless steel if you ever work with it.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  5. #5
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Ah yes, the nozzle spray, thanks. I do have straight Ar, one of the reasons I gave up even trying to dial in.

    I don't think I ever touched the 308 from when I stocked for TIG, so I'll skip that for now.

    I'll have to do a bit more research on the hardfacing, hope it won't be too picky about the gas. I sorta doubt they stock it anyway.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  6. #6

    Default

    Extra contact tips of .023, .030 and .035. Nozzle spray or dip work, or PAM. Did you get a spool gun? 4043 probably will not feed well.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  7. #7
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by everlastsupport View Post
    Extra contact tips of .023, .030 and .035. Nozzle spray or dip work, or PAM. Did you get a spool gun? 4043 probably will not feed well.
    Yep, the SM-200N. I hope you don't mean that it wont feed well from the spoolgun.

    Got a couple surprises at the store, price to buy a cylinder was WAY up from a year ago, but the rest of the steff didn't add up to as much as I thought.

    And LWSs don't seem to stock much in the way of Binzel parts. Time to make an order from China I guess. Looks like liners are quite cheap there, might as well get some. How long do they usually last?
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  8. #8

    Default

    Quote Originally Posted by redbeard View Post
    Yep, the SM-200N. I hope you don't mean that it wont feed well from the spoolgun.

    Got a couple surprises at the store, price to buy a cylinder was WAY up from a year ago, but the rest of the steff didn't add up to as much as I thought.

    And LWSs don't seem to stock much in the way of Binzel parts. Time to make an order from China I guess. Looks like liners are quite cheap there, might as well get some. How long do they usually last?
    You will want a spool gun to feed 4043, will not feed well without.

    I have a 5+ year old binzel that has the original liner. And has feed flux and solid wire. But wire is always clean since it is used a few times a week. No wire cleaner either.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. IMig 140 Power Supply
    By ChuckD in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 11
    Last Post: 09-13-2014, 06:12 AM
  2. 200DX Consumable starter pack
    By zedron in forum Pre-sales, Sales and Shipping questions
    Replies: 16
    Last Post: 01-03-2013, 05:27 PM
  3. Consumables starter pack.
    By AWDnot2 in forum Pre-sales, Sales and Shipping questions
    Replies: 0
    Last Post: 11-01-2012, 01:14 PM
  4. HF Arc Starter with PA 200?
    By BorderBrewer in forum Stick Welding (SMAW)
    Replies: 7
    Last Post: 08-09-2012, 05:03 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •