Share
Results 1 to 7 of 7

Thread: Arc welding and pacemakers

  1. #1

    Default Arc welding and pacemakers

    I love to arc weld. I have a few machines and they all have their uses. I have my dad with me and he has had heart bypass with a pacemaker. There are warnings about arc welding and pacemakers so I decided to look into the warnings so my dad would feel at ease.

    As it turns out, you can weld around someone with a pacemaker. But if you have a pacemaker, then arc welding may be something to reconsider. The danger zone to a pacemaker to an arc weld is 18 to 24 inches. About where a person needs to be to weld. A person can be in the room when arc welding but keep them at lest 2 feet away from any arc.

    Here is a link to a study done about arc welding and pacemakers.....http://www.sta-tn.com/IJ_STA/Papers/.../IJSTA_211.pdf

    And here is a link to the AWS (American Welding Society) about pacemakers and welding.http://www.aws.org/wj/amwelder/9-00/safety.html
    Powertig 250EX
    Powerplasma 50
    Hobart Handler 210 with spoolgun
    Cobra 2000 / Henrob O/A torch
    Drill press / metal brake / 36 ton air hydraulic press
    Franzinated modified Craftsman 33 compressor
    Lots of other metal working tools

  2. #2

    Default

    Great info good to check better safe then sorry

    Everlast PM256
    Millermatic 180
    Hypertherm PowerMax 65 with machine torch
    Longevity Force Cut 80I
    DIY CNC table for plasma/routing
    13" metal lathe
    Small Mill
    ect, ect.

  3. #3
    Join Date
    Jan 2010
    Location
    Milton FL Was from San Rafael CA
    Posts
    16

    Default

    I have purchased quite a few pices of equipment from Alex
    as of 6/14/13 I can not use due to a pacemaker
    I build street rod parts and weld
    I am Here By Gods Grace

  4. #4

    Default

    I have a pacemaker and have no problems with mig tig and stick. My normal testing and data transmission from my implant shows no problems. My Cardiologist main concern was not welding but magnets or anything that generates a magnetic field. His first question was about firearms he wanted to know if i shut right handed or left as the impact from a shotgun could break my wires or damage my implant. Some of the older pacemaker defibrillator's run at frequency's that can have an interference problem.

    I have had no problems as i weld a lot and my pacemaker runs approximately 3.5 hours per a 24 hour period.
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  5. #5

    Default

    The main concern has been TIG with High Frequency from what I've been told. I've also been told they make shielded pace makers just for these type applications, but are more expensive??

  6. Default

    A pace maker is not a pace maker is not a pacemaker. By that I mean that are several types. There are pace makers that completely control the heart. There are demand pacemakers that only kick in if the heart rate drops below a certain rate. And there are defibrillators, they are for shocking a heart out of a dangerous rhythm. The only one that really has the most potential for problems is the first one because it is working 100% of the time.

  7. #7

    Default

    Not sure I would want the defib model zapping me while welding either though. I have seen out MIGs as well interfere with the TV signal. So I would probably talk to the heart guy first. Safety first.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. First Welding Project - You guessed it... a welding cart
    By EmptyNester in forum Hobyist Projects
    Replies: 19
    Last Post: 10-12-2011, 04:30 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •