Figure about 5 minutes on and 5 minutes off. Normally you need more filler or ER, so the delay to get another rod might work where you are working 100% though yours power at 50-60% duty cycle wise.
 
 
		Figure about 5 minutes on and 5 minutes off. Normally you need more filler or ER, so the delay to get another rod might work where you are working 100% though yours power at 50-60% duty cycle wise.
Mike R.
Email: admineverlast@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x203
M-F 12 - 7PM PST
FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.