Share
Results 1 to 7 of 7

Thread: MIG wire cleaner

  1. Default MIG wire cleaner

    My MIG wouldn't feed unless the tensioner was cranked all the way up. A professional welder showed me how to insert the wire through a foam ear noise plug (the kind you stick in your ear) between the MIG roll and the tensioner. The foam wipes the wire prior to entering and keeps the roller from gumming up with the protective coating on the wire. No more slippage.

  2. #2

    Default

    Good mig wire won't have anything on it since that's what the copper is for. I've seen flux core wire with some gunk on it. I use these Click image for larger version. 

Name:	mig pads.jpg 
Views:	772 
Size:	86.0 KB 
ID:	10114

    Why two threads on the same subject ?
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #3

    Default

    Quote Originally Posted by zoama585 View Post
    Click image for larger version. 

Name:	mig pads.jpg 
Views:	772 
Size:	86.0 KB 
ID:	10114
    Hard to tell from the picture but felt pads in a spring clamp?

  4. #4

    Default

    Quote Originally Posted by Mr120 View Post
    Hard to tell from the picture but felt pads in a spring clamp?
    Yes, one cleans and the other lubricates. Both are used at the same time. http://store.cyberweld.com/weaidlucopak.html
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  5. #5
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by zoama585 View Post
    Good mig wire won't have anything on it since that's what the copper is for. I've seen flux core wire with some gunk on it. I use these Click image for larger version. 

Name:	mig pads.jpg 
Views:	772 
Size:	86.0 KB 
ID:	10114
    Looks exactly like what I saw on the Steve Bliel video. After I watched it, I ran right out and cut a strip off a scotch-brite sanding pad and attached it with a clothes pin.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  6. #6

    Default

    Quote Originally Posted by redbeard View Post
    Looks exactly like what I saw on the Steve Bliel video. After I watched it, I ran right out and cut a strip off a scotch-brite sanding pad and attached it with a clothes pin.
    I wouldn't want grit getting into the liner. The purpose is to clean the wire and stop copper from being rubbed off inside the liner. Two dollars and change ain't much.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  7. #7
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by zoama585 View Post
    I wouldn't want grit getting into the liner. The purpose is to clean the wire and stop copper from being rubbed off inside the liner. Two dollars and change ain't much.
    These are the pads used between coats for wood finishes, they don't seem to be gritty at all. If they were , I wouldn't have chanced trashing the rollers. I agree, that isn't much to spend for the proper product, I just didn't know it existed until this thread.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

Similar Threads

  1. Tig welding with magnets around and aluminum cleaner
    By Steve in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 08-05-2013, 06:21 PM
  2. MIG wire cleaner
    By Schuh in forum Technical Bulletins and Tips
    Replies: 1
    Last Post: 06-09-2013, 12:44 AM
  3. Brake Cleaner Phosgene Gas
    By dwdw in forum General Welder Questions
    Replies: 27
    Last Post: 04-02-2013, 08:52 AM
  4. Replies: 26
    Last Post: 02-22-2012, 11:25 AM
  5. "Ultra Bright Aluminum Cleaner" acid-based aluminum cleaner review
    By jakeru in forum General Welding Questions
    Replies: 4
    Last Post: 06-29-2011, 07:02 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •