    First off, I'd like to say thanks for the fast shipping, the welder got here before the tracking number did! Kudos to Reddaway, they were just as fast as either of the parcel services.

    Couple of disappointments, first, the regulator was missing. Second, nothing happened when I pulled the trigger. After a bit of troubleshooting, it seems that the pins in the euro connector are not making contact. Not sure why the spool gun connector (on the left in the pic) makes contact, but the other one doesn't. Hopefully I'll get some time to figure it out this afternoon.
    Click image for larger version. 

Name:	DSCN1783.jpg 
Views:	376 
Size:	123.7 KB 
ID:	10099Click image for larger version. 

Name:	DSCN1789.jpg 
Views:	443 
Size:	121.4 KB 
ID:	10100

    Is there an updated manual available that I missed? The one on the manuals page is really outdated (and doesn't cover pulse) and I gave up trying to understand the Chinglish one in the crate after about 3 sentences. The most immediate question though, is how do I set the wire speed? Or did this thing go synergic when I wasn't paying attention?
    Click image for larger version. 

Name:	DSCN1778.jpg 
Views:	393 
Size:	129.3 KB 
ID:	10098
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  2. #2

    Default

    Amps = wire speed. I believe it reads wire speed when idle and actual amps when welding. Which spool gun did you get ? A pic of the whole spoolgun setup would be nice.
    Last edited by zoama; 06-08-2013 at 05:57 PM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #3

    Default

    Tighten your liner nut down or check to see if the liner is too long. Looks like it is sticking up too high.

  4. #4
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by zoama585 View Post
    Amps = wire speed. I believe it reads wire speed when idle and actual amps when welding. Which spool gun did you get ? A pic of the whole spoolgun setup would be nice.
    I do remember the pics of the old unit with the dial labeled Wire Speed/Stick Amps. Not sure why it is labled straight up as MIG amps with the correction factor for stick amps off to the side now. The range at idle is 55(actually speed, 0 IPM) to 286 (actual speed not yet tested). Maybe after some futzing around I'll get it all figured out.

    I went with the SM200. Seems pretty well built and it was plug and play. Sweet! Only downside is that the speed is not controlled at the gun. Mark, I think you mentioned a while back that could be fixed with some rewiring, might you happen to remember where that info is?
    Click image for larger version. 

Name:	DSCN1808.jpg 
Views:	388 
Size:	141.1 KB 
ID:	10108 Click image for larger version. 

Name:	DSCN1805.jpg 
Views:	405 
Size:	137.2 KB 
ID:	10107 Click image for larger version. 

Name:	DSCN1804.jpg 
Views:	403 
Size:	133.7 KB 
ID:	10106

    Thanks Mark, I'll check that in the AM. I tweaked the pins in a bit and got it working, but doing it that way didn't seem right to me.

    Even after laying just a couple bead-like formations, I can tell already I'm gonna like MIG and this machine in particular. Wish I didn't have to wait till Thursday to get supplies and get going with it. Guess that does give me more time to watch Jody's MIG collection though.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  5. #5

    Default

    Quote Originally Posted by redbeard View Post
    [snip]Only downside is that the speed is not controlled at the gun. Mark, I think you mentioned a while back that could be fixed with some rewiring, might you happen to remember where that info is?[snip]
    Try here:

    http://www.everlastgenerators.com/fo...6521#post46521

  6. #6
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by Mr120 View Post
    Ooh thanks, I completely missed that thread's revival. Guess I should make more of an effort not to go AWOL.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  7. #7

    Default

    Very nice. I need a spool gun.
    Purple Fabricator 211i

  8. #8
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by 225 View Post
    Very nice. I need a spool gun.
    I was pleasantly surprised that it is 25', 25% longer than the advertised length, cool! I don't care much for the denim cover though, it gets impregnated with dust & dirt in no time.

    The liner was a bit long, trimming improved the situation, but it is still a bit finicky, not 100%.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  9. #9

    Default

    Quote Originally Posted by redbeard View Post
    I was pleasantly surprised that it is 25', 25% longer than the advertised length, cool! I don't care much for the denim cover though, it gets impregnated with dust & dirt in no time.

    The liner was a bit long, trimming improved the situation, but it is still a bit finicky, not 100%.
    Is the neck and nozzle energized on yours when you weld ? You could check with a multi meter without shorting it.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  10. #10
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by zoama585 View Post
    Is the neck and nozzle energized on yours when you weld ? You could check with a multi meter without shorting it.
    Is yours? I just checked for continuity and there is none between the tip and nozzle. I'm also pretty sure I drug it when testing, and nothing scary happened.

    Just discovered another plus, they both use the same consumables. Now I wonder if the necks are interchangeable too.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  11. #11

    Default

    Quote Originally Posted by redbeard View Post
    Is yours? I just checked for continuity and there is none between the tip and nozzle. I'm also pretty sure I drug it when testing, and nothing scary happened.

    Just discovered another plus, they both use the same consumables. Now I wonder if the necks are interchangeable too.
    The mig torch that came with my 250 had the nozzle energized so it would burn away or stick if it touched in a corner.
    I'm not complaining at all, just curious about the spool gun after kempy said his neck and nozzle were always hot on the same model spool gun. I'm gonna buy one soon.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  12. #12
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by zoama585 View Post
    The mig torch that came with my 250 had the nozzle energized so it would burn away or stick if it touched in a corner.
    I'm not complaining at all, just curious about the spool gun after kempy said his neck and nozzle were always hot on the same model spool gun. I'm gonna buy one soon.
    Makes me think he might have exceeded the duty (200A@35%) and melted through the internal insulation. It might explain some of the problems he has been having and why it was fine when he first got it.
    Since it has been said that this is basically the same gun as the Miller Spoolmate 200, that is further rated at 160A@60%. I can see how it might be easy to exceed that.
    It might be time to produce a 300A spoolgun for some of the more powerful welders, like Lincoln does.
    Long arc, short arc, heliarc and in-the-dark!

  13. #13
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by Rambozo View Post
    Makes me think he might have exceeded the duty (200A@35%) and melted through the internal insulation. It might explain some of the problems he has been having and why it was fine when he first got it.
    Since it has been said that this is basically the same gun as the Miller Spoolmate 200, that is further rated at 160A@60%. I can see how it might be easy to exceed that.
    It might be time to produce a 300A spoolgun for some of the more powerful welders, like Lincoln does.
    It could be something as simple as a little chunk of clipped wire that fell into the neck as well. Either way, a disassemble and inspect should reveal what is up.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

Similar Threads

  1. Imig 205//210
    By Doc Pete in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 2
    Last Post: 01-19-2017, 11:25 AM
  2. Problem with Imig 205
    By Chris A in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 13
    Last Post: 06-08-2014, 12:16 PM
  3. A few welds with my IMIG 200...
    By CGCINC in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 20
    Last Post: 07-16-2012, 11:42 AM
  4. Power I-IMIG 250P questions
    By Diabolical in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 11
    Last Post: 02-13-2012, 09:05 PM
  5. Imig 200 Question
    By SeanMurphy265 in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 1
    Last Post: 08-01-2011, 01:16 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •