Ok I opened my unit and the first things I noticed...

The TIG SIDE:
I am really disappointed in the torch. My TIG torch looks like the chap ones you get on ebay. It is not the blue handle one you see on the website description and are lead to believe you are getting, nor is it the one that Jody demoed in his video. The flow meter is basic and functional but is in LPM.

STICK SIDE:
I like the sturdiness if the stinger.

ELECTRICAL:
The unit is wired with a 220 plug but I can not see what amps it is. I was told in the forums to not use it an to change it out for a 220/50 plug. It also has the 220 to 110 pigtail.