Pool season again and since I'm the "pool boy" at our Villas, I decided I wanted some plants to make it more homey....
I found the huge Elephant Ear tree at a local store but couldn't find a planter big enough or heavy enough to not tip over so I made one out of concrete.
Bought the tree on a Sunday and the pool opened the following Saturday so I had less than a week to make the forms, pour the concrete and hope it would dry fast enough to hold together moving it from my shop to the pool.
I used 4.5 bags of concrete @ 80lbs.....2 bottles of Charcoal tinting and some Malamine shelving I had sitting around.
I had a little chipping pulling the forms and moving it but it turned out fine.
![]()