My neighbor, Mario, asked me reattach the legs to his cast iron Rooster that had been broken.
https://dl.dropboxusercontent.com/u/...9/P1010589.JPG
https://dl.dropboxusercontent.com/u/...9/P1010592.JPG
Used my 256PP and preheated it and used 70s2 filler.