The switch on my new torch stopped working.
Swapped to the pedal and the welder worked fine.
Took the switch backing plate off, and it all looks fine then noticed it would work occasionally depending on where/how the switch was held.
It's acting like there is a break in the wire somewhere. Like i said, the actual switch looks fine, the connections are solid, and I can feel the depression and hear the 'click' sound.
If I order a new switch, do you know if it will come with the full length wire or just the switch? Does anyone know what size wire is used< would make sense to try a new length of wire to rule out a broken wire.
Frustrating to say the least.