So far I'm very pleased with it, the arc was very smooth and stable and the pulse is great. I just need to get better consumables, Ive always used a gas lens, but none of my consumables fit, so I tried to weld with what came with the torch... I used the wrong cup for the wrong application and porosity city! I've never had porosity with tig welding, so imagine my surprise! lol I'll be heading to the store to get the right consumables, which is what I should have done in the first place.
Once I get it going correctly, I'll do a video review, showing off the unit. I have to get used to welding with an inverter machine though, as I have always used a transformer type.


 
					
					 
							