Originally Posted by
jimmy
I have a PowerPro 205, let me know if I can weld aluminum with stick mode and if you can give me tips on how to weld
thank who can help me!!
I tried stick welding aluminum it is very dirty and smoky but it works, I rather Mig or Tig aluminum you have a good Tig welder. the videos that Mr120 and DaveO are very good also good luck. Which aluminum stick rod are you going to use.