    Question stick welder aluminum

    I have a PowerPro 205, let me know if I can weld aluminum with stick mode and if you can give me tips on how to weld
    thank who can help me!!

  2. #2

    Default

    Interesting that you should post this question. I was checking out the Everlast channel (great channel by the way) and saw this video:

    http://www.youtube.com/watch?v=UY7KAnJGYwY

    More like a specialty welding process. Check out their other videos too. I'm not sure why the Everlast youtube videos aren't being posted in this forum.

  3. #3

    Default

    Quote Originally Posted by Mr120 View Post
    Interesting that you should post this question. I was checking out the Everlast channel (great channel by the way) and saw this video:

    http://www.youtube.com/watch?v=UY7KAnJGYwY

    More like a specialty welding process. Check out their other videos too. I'm not sure why the Everlast youtube videos aren't being posted in this forum.
    Many of them are, but I guess we need a collective area/thread to post them.

    As far as welding aluminum goes. It's not cheap. It's about 20-30/lb. And a pound lasts about 15 minutes if you are sticking it together...but you are moving almost faster than you could MIG it.

  4. #4
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    How about a Video menu item or a button on the site that takes you to the Everlast YouTube channel? Something that shows up on the homepage as well as from the forum pages. There is the video library link under resources, but it looks like everything is moving to YouTube, so linking right to the channel makes sense. Also that menu isn't accessible from the forum pages. Maybe something can go under Quick Links. By linking to the channel you wouldn't have to worry about updating individual video links or some long sticky thread with all of them.
    Long arc, short arc, heliarc and in-the-dark!

  5. #5
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Because the 205 is also a DC stick welder, you can weld aluminum with aluminum stick electrodes. Some more information about it here- the author uses an Everlast machine:
    http://www.hildstrom.com/projects/st...num/index.html

    Post up some photos if you give this a try!
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  6. #6
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Quote Originally Posted by jimmy View Post
    I have a PowerPro 205, let me know if I can weld aluminum with stick mode and if you can give me tips on how to weld
    thank who can help me!!
    I tried stick welding aluminum it is very dirty and smoky but it works, I rather Mig or Tig aluminum you have a good Tig welder. the videos that Mr120 and DaveO are very good also good luck. Which aluminum stick rod are you going to use.
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  7. #7
    Join Date
    Nov 2012
    Location
    san jose, costa rica
    Posts
    8

    Default

    tanks for your help!!!!
    I will watch the video. I hope to be helpful

Similar Threads

  1. wanting to buy stick welder
    By johnson697 in forum Stick Welding (SMAW)
    Replies: 4
    Last Post: 09-07-2017, 07:05 AM
  2. Power I Mig 200 MIG STICK WELDER , how high should the amp gauge read on stick side
    By Tim L Rogers in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 01-22-2016, 04:42 AM
  3. Mystery Welder Revealed: 2012 DIGITAL POWERTIG 210EXT TIG/STICK welder
    By performance in forum Everlast Announcements, Contests and Promotions
    Replies: 46
    Last Post: 07-28-2012, 02:19 AM
  4. using a coiled mig gun in place of the arc stick welder
    By britstef in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 7
    Last Post: 07-17-2010, 12:38 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •