Share
Results 1 to 3 of 3

Thread: Issues (Yellow) Supeer Pro 160, will not switch between modes

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default Issues (Yellow) Supeer Pro 160, will not switch between modes

    Good morning Gents..... I have one of the older SuperPro 160s, back when everything was still yellow..haha

    Anyhow, I love my machine but have had a couple of issues lately. I figured I would ask here and see what other folks know.

    The initial problem is, I'm unable to switch my machine between modes. Its like its stuck on Plasma cutter. Also, while in plasma cutter...the trigger will not activate the air side of the equation. When you squeeze the trigger all that happens is you can watch the AMPs go up in the display.

    Any suggestions would be most appreciated.

    Heath
    Last edited by hhubred; 04-24-2013 at 05:04 PM. Reason: better title

  2. #2

    Default

    Don't remember a "super pro"
    But sounds like your solenoid is stuck, and possibly a switch is worn out on the surface. Other than that you can send it in for repairs. Sounds like the warranty is probably out on that old of a machine.

  3. #3

    Default Issues (Yellow) Super 160P, will not switch between modes

    Your right..... Its a Super 160P.

    I was able to work the switch back and for between Stick and Tig, until I saw the Amps come up for stick welding. Once I did it a couple of times it started switching modes with ease. Probably not the most technical fix but it worked for me.

    The Plasma cutter has a loose connection somewhere in the switch at the cutter end. I was able to play with it enough to work for a little while longer. Is there a replacement switch for this?

    Heath
    Last edited by hhubred; 04-26-2013 at 12:02 AM.
    Heath
    Belton, Tx
    Super 160P

Similar Threads

  1. i-TIG 201 power switch problems
    By BillN in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 12-31-2017, 06:09 AM
  2. On/off switch issues
    By broberts5 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 08-16-2013, 11:53 PM
  3. Pedal switch
    By WikingWelder in forum Other Custom Fabrications
    Replies: 14
    Last Post: 04-16-2013, 11:08 AM
  4. Welding a zinc yellow plated grade 8 bolt
    By ShaneJackson in forum General Welding Questions
    Replies: 6
    Last Post: 10-24-2012, 10:00 PM
  5. switch
    By ewest30 in forum Everlast Plasma Cutters (PAC)
    Replies: 7
    Last Post: 11-03-2009, 12:22 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •