Share
Results 1 to 19 of 19

Thread: Another Cracked Regulator

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Exclamation Another Cracked Regulator

    I know I'm not the only one with this problem... and I'm sure Everlast is addressing this. But these regulators (Model GH-25 made by the Zhejiang Bril company in China are downright dangerous - mine split right down the middle (see pic)!!! If you have one of these regulators keep a close eye on it if it's not leaking. Personally, I'd pitch it in the nearest dumpster!Click image for larger version. 

Name:	Crack in Regulator.jpg 
Views:	608 
Size:	133.4 KB 
ID:	10059

  2. #2

    Default

    We've changed regulator suppliers recently and most all the new ones are made from billet brass. This is the older style. If yours is less than 6 months, we can send you another unit.

    On the other hand, I've got one of those I've had for nearly 4 year now. No issues.

  3. #3

    Default

    Quote Originally Posted by performance View Post

    On the other hand, I've got one of those I've had for nearly 4 year now. No issues.
    I have a few of them even older (about 4 in use). Just gave my first one away with an IMIG-200 and 131 tank.

    Maybe it was dropped somewhere along the way or over torqued at the factory. How old is it?

    We have had a couple cracks over the years, but we have sold way more than a couple welders.

    But either way, that needs to be remove ASAP, it could be really dangerous. Call Oleg and see what he can workout for you. I have used the local HF ones, Clarke knock-off if you need one this weekend in a hurry. If on sale, and a 20% off coupon they can be had for about $26-28 dollars.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  4. #4

    Default

    I tossed my regulator the day the 250EX arrived as I didn't trust it and bought a Smith instead. I bought the 250EX for the machine alone and it's been behaving ever since.
    Millermatic 251 with 30A
    Synchrowave 180
    Hobart 100 MIG
    lathe & RF45
    Power TIG 250EX
    Spectrum 625 X-TREME
    Spray Zone.net-Side draft spray booth

  5. #5

    Default

    I've got 3 of the chrome regulators and never had a problem other than a blown pressure gauge. The new ones may be higher quality, but old design allows you to make a dual flowmeter for purge. Click image for larger version. 

Name:	IMG_1197.jpg 
Views:	461 
Size:	130.7 KB 
ID:	10061
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  6. #6
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Be careful out there, folks!

    Quote Originally Posted by everlastsupport View Post
    ...
    We have had a couple cracks over the years, but we have sold way more than a couple welders.

    But either way, that needs to be remove ASAP, it could be really dangerous. ...
    Mike, I'm surprised that you're only aware of "a couple" cracked Everlast flowmeters.

    Over a year ago, I informally counted (and provided links to) six different forum members reporting cracked Everlast flowmeters in this related post:
    http://www.everlastgenerators.com/fo...8076#post18076 {/quote]
    '13 Everlast 255EXT
    '07 Everlast Super200P

  7. #7

    Default

    Quote Originally Posted by jakeru View Post
    Mike, I'm surprised that you're only aware of "a couple" cracked Everlast flowmeters.

    Over a year ago, I informally counted (and provided links to) six different forum members reporting cracked Everlast flowmeters in this related post:
    http://www.everlastgenerators.com/fo...8076#post18076 {/quote]
    I didn't mentioned, we did have a bad batch of them "at one time" awhile back, as that was a unique case. And we handled that, sometimes we do have an issue like other companies, but all in all there is no problem with the regulator. And as always we resolved any problems. It was something sort of beyond our control.

    Either way, I still use mine, and mine are even older than Mark's.

    Also, I hope everyone knows to be careful when you turn on the tank, as hoses can blow off as well. I always stand on the other side of the regulator and hose. Always use caution when cracking the valve, I turn it on slowly then open it up. Just a habit, nothing to do with our regulator, just a safer way to do it.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  8. #8
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by everlastsupport View Post
    Also, I hope everyone knows to be careful when you turn on the tank, as hoses can blow off as well. I always stand on the other side of the regulator and hose. Always use caution when cracking the valve, I turn it on slowly then open it up. Just a habit, nothing to do with our regulator, just a safer way to do it.
    Good tip Mike, I always try to open it slowly, but never much thought about standing out of the line of fire. Just like standing to the side of your bench grinder when you hit the switch.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  9. Default

    As usual you guys are right on top of things. I just posted the picture for other users that might still have these units. Clearly this supplier had issues! Cheers!!!

  10. #10

    Default

    I have this style for my 200dx and just received (but haven;t yet tried) a new 185 with the newer regulator. New regulator looks nice. Haven;t had any issues with the onl one other than a bit of a high pressure burst each time I start an arc (I pre-purge before striking).
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  11. #11
    Join Date
    Oct 2010
    Location
    Nova Scotia, Canada
    Posts
    143

    Default

    My Aire Liquide one does that too. It's got nicer (and maybe smaller diameter) hose which helps though.

    Builds up about 30 psi on the low pressure side when switched off with a fresh tank.

  12. #12
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Paul Moir View Post
    My Aire Liquide one does that too. It's got nicer (and maybe smaller diameter) hose which helps though.

    Builds up about 30 psi on the low pressure side when switched off with a fresh tank.
    The fix is to use a short, small diameter, and as non-ballooning hose as possible. Also you can add an orifice to help limit peak flow. There is a company that sells a gas saver system for TIG and MIG that does just that.

    http://www.netwelding.com/How_GSS_Works.htm

    In the past I've used braided stainless teflon hose for argon. It works great and was leftover from plumbing a race car.
    Long arc, short arc, heliarc and in-the-dark!

  13. #13
    Join Date
    Oct 2010
    Location
    Nova Scotia, Canada
    Posts
    143

    Default

    That's an idea. The AL one is reinforced rubber and might be 3/16".

    Another idea is to relocate the gas solenoid up onto the regulator. IIRC on my 225LX it's a 240v solenoid, so that's a little tricky.

    Fortunately I don't pay for the gas. Well, directly anyway. So I'm pretty content with just a bit of preflow to miss the blast.

    When I finally build a cart, maybe I can do something about the hose length eh?
    Last edited by Paul Moir; 05-26-2013 at 03:36 AM.

  14. #14

    Default

    Jake

    In 2012 we sold around 8k units
    And possibly exchanged 30-50pc
    Of regulators, maybe I am wrong, but I don't think it's called for massive recall
    All costumers reported any issue once they start using the welder.

    Oleg
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  15. #15

    Default

    Additionally, all accessories are covered by a 6 month warranty, including regulators, foot pedals, torches, and clamps.

  16. #16
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Regulator for MTS250S plugged with thread sealant when I was going to use a second bottle with different gas I thought I would use to regulators and a Y manifold but it would not flow took it apart and the tank inlet was full of sealant.
    Click image for larger version. 

Name:	regulator inlet pluged with sealer.jpg 
Views:	462 
Size:	151.4 KB 
ID:	10120
    Model GH-25
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

Similar Threads

  1. New regulator
    By dzljon in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 12-21-2014, 06:27 PM
  2. Regulator rebuild
    By DaveO in forum Personal Projects (no welder required)
    Replies: 0
    Last Post: 01-02-2013, 01:11 AM
  3. Replies: 3
    Last Post: 06-18-2011, 07:32 PM
  4. Cracked right in the middle of the aluminum weld
    By DiabolicZ in forum TIG Welding (GTAW/GTAW-P)
    Replies: 18
    Last Post: 03-24-2011, 07:11 PM
  5. regulator
    By bobkat in forum Customer Testimonials
    Replies: 1
    Last Post: 03-11-2011, 10:18 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •