I have my welder hooked up on a 220 outlet, Just came in the mail and just started getting set up. Just practicing on small piece of aluminum strap. Pure argon gas.
On pulse mode should the digital display jump so much??131 63 132 78 and so on
I can only make about 5 passis across 1 1/4 x 3/16 aluminum strap and the welder kicks into a limp mode. Not familiar with tig welders. but is there supposed to be that spark inside the welder itself? and thats about what I get out of the tip to material when it kicks out just a little wimpy spark not a weld arc.
When I let it cool and reset the breaker on the welder It welds perfectly otherwise.
Just trying to get to know the product.
Not watercooling the torch yet either. But im making very small welds and taking time between. Would this affect much besides consumables being used up?