  1. Default 256 Plasma Question

    I have a Everlast 256 that I use mostly for Tig. It tig welds great. I don't use the plasma cutter much so I must be doing something wrong.

    Cutting 3/16 plate, Voltage set at 38, Air PSI 60, Torch is in the postive port. The air is dry and coming from an 8 hp compressor with a 60 gal volume tank. All of my green knobs are shut off and the machine is switched to cut.

    The pilot ark works fine. The torch will cut 18 gauge fine. As a test I cut the numbers 1 2 3 4 in sime 18 gauge and it cuts like butter.

    When I try to cut the 3/16 the torch cuts about 1/3 the way through and then does not seem to penetrate any further. I tried restarting, letting the edge heat up like you would if using a small cutting torch but it would not cut through. The work clamp has a good connection to the work.

    Click image for larger version. 

Name:	Plasma cut 1.JPG 
Views:	532 
Size:	123.6 KB 
ID:	9886Click image for larger version. 

Name:	plasma cut 2.JPG 
Views:	542 
Size:	130.2 KB 
ID:	9887

    The angle iron and clamps are my guide. But you can see it did not cut all the way through. Cuts the thin metal with no problems.

    Any ideas are greatly appreciated.

    Bill

  2. #2

    Default

    What torch/ Unit do you have? 2013?

    Torch is in WRONG port. Have you downloaded and fully read the manual located online on our site under the manuals section at the top?

    Air pressure sounds low and you'd need to turn up the amps to max to get the best test.

  3. #3

    Default

    You're only cutting with the pilot arc due to the torch being in the wrong port. Post a picture of your torch please.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  4. #4

    Default

    You may have also damaged your torch by using the wrong polarity...definitely probably toasted a consumable.

  5. Default

    Mark:

    I will look when I get to the shop tomorrow.

    thanks,

    Bill

  6. Default

    I made a mistake in my original post. The tourch was connected to the (-) port. All I did was disconnect my tig tourch and plug in the Plasma. I was hopping it was something simple like opperator error.

    It mey be tomorrow before I can post a picture of the tourch.

    Thanks,

    Bill



    Quote Originally Posted by wheelrdealer View Post
    I have a Everlast 256 that I use mostly for Tig. It tig welds great. I don't use the plasma cutter much so I must be doing something wrong.

    Cutting 3/16 plate, Voltage set at 38, Air PSI 60, Torch is in the postive port. The air is dry and coming from an 8 hp compressor with a 60 gal volume tank. All of my green knobs are shut off and the machine is switched to cut.

    The pilot ark works fine. The torch will cut 18 gauge fine. As a test I cut the numbers 1 2 3 4 in sime 18 gauge and it cuts like butter.

    When I try to cut the 3/16 the torch cuts about 1/3 the way through and then does not seem to penetrate any further. I tried restarting, letting the edge heat up like you would if using a small cutting torch but it would not cut through. The work clamp has a good connection to the work.

    Click image for larger version. 

Name:	Plasma cut 1.JPG 
Views:	532 
Size:	123.6 KB 
ID:	9886Click image for larger version. 

Name:	plasma cut 2.JPG 
Views:	542 
Size:	130.2 KB 
ID:	9887

    The angle iron and clamps are my guide. But you can see it did not cut all the way through. Cuts the thin metal with no problems.

    Any ideas are greatly appreciated.

    Bill

  7. Default

    Quote Originally Posted by zoama585 View Post
    You're only cutting with the pilot arc due to the torch being in the wrong port. Post a picture of your torch please.
    Click image for larger version. 

Name:	torch 01.JPG 
Views:	549 
Size:	119.1 KB 
ID:	9901Click image for larger version. 

Name:	torch 02.JPG 
Views:	535 
Size:	106.8 KB 
ID:	9902

    Zoama585:

    Here are the pictures of the torch. The consumables are toast. I have replacements but wanted you to see the torch as it was after the attempted cut.

    Any ideas are appreciated.

    BR

  8. #8

    Default

    isn't there supposed to be a ceramic cup on the end?
    pn# cv0076 in the manual?

  9. #9

    Default

    Wow, never thought about running a torch without the ceramic shield, but I would bet that is what it might look like. Kinda like Chernobyl, without the containment (Sorry Oleg).

    I think if the polarity were reversed, the actual nozzle would not even be there anymore. Like a TIG torch would melt away the Tungsten.

    I bet Gman is right, assembly issue?
    Last edited by Big Paulie; 04-12-2013 at 03:38 PM. Reason: Spelling
    Everlast PowerPro 256 (2013)
    Northern Hybrid 200 & ST80i
    HF 90Amp FluxCore (Don't laugh, it is what got me started)
    Lotos LT5000D Plasma
    HF 4x6 Horizontal Bandsaw
    Rikon 18" Bandsaw w/VFD
    Delta 14" Drill Press
    Robland NLX31 Euro Combo WW

  10. #10

    Default

    What does your swirl ring look like?

    Check the cables in the work clamp and the work clamp dinse and GRIND an area for the work clamp to attach.

  11. #11

    Default A81 Torch??

    The pictures look like my A81 torch that I ordered as an option with my PP256. My A81 has a label by the trigger on the LEFT side of the torch which states it is an A81. My unit also came with a “flow gauge” to set the volume of air through the torch. Very DRY air is needed to keep the consumables happy. 60 psi is too low for the A81 torch.
    Everlast PowerPro 256
    Everlast W300 Cooler
    Everlast Cart 250

    Millermatic 211
    Spoolgun 100
    Miller HD Cart

    Victor 315 Torch sitting on a Harper 830-86 cart

  12. #12

    Default

    Make sure the swirl ring is there and right side up. Also, the containing nozzle is on the torch. And it is a little toasty.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  13. Default

    Quote Originally Posted by everlastsupport View Post
    Make sure the swirl ring is there and right side up. Also, the containing nozzle is on the torch. And it is a little toasty.

    Here is the A81 disassembled, new consumables ready to install. Any suggestions on where to start to correct this problem? What is a good basic starting set up for 3/16 mild steel? I have a peice of 3/16th I need to cut an arch in for a frame fishplate. Would like to do it with a plasma versus the zip wheel and grinding it down to final shape.

    Click image for larger version. 

Name:	torch 3.JPG 
Views:	537 
Size:	135.4 KB 
ID:	9903

  14. #14

    Default

    Amps can be low for 3/32" if you like. Make sure the swirl ring has the holes toward the tip/electrode, not the torch. Air pressure around 72 should be fine. The bad consumables, Mark might want to chime in, are you sure you have no moisture in the tank? Do not worry about the nozzle, I've gotten in corners and had blow back mess them up, they still will work fine.

    For the guys that asked about the nozzle, lower left corner, looks a little rough. I would grind the end smooth (black part off)
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  15. #15

    Default

    Please note that air pressure needs to be 72 psi while cutting. The pressure will be higher when the air is not flowing. To set the working pressure, turn the postflow to max, then with the torch pointed in a safe direction, tap the trigger just long enough to start the air flowing and adjust the regulator to maintain 72 psi while the air is flowing. After setting the pressure, return the postflow to about 10 seconds to prolong the life of your consumables. I'd use about 35 amps cutting 3/16. Move the torch as fast as it cuts through for the cleanest cut. The faster you move the torch without skipping, the cleaner your cut will be.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  16. #16

    Default

    There's no harm at running at max amps or close to it. The problem with lower amperage is that you have to drop down in size of the orifice to get the most stable arc and highest quality cut. The cut tips are probably good for up to 80 amps, so at 60, you are already down on amperage. Going lower can really start to affect cut quality. A higher amperage cut will also be a faster cut.

  17. Default

    Thanks , I never thought about using post flow to set the air flow. All good suggestions I will try them tomorrow.

    Mark

    Thanks for the advice I will try it tomorrow.

    Thanks

  18. #18

    Default

    Just to be clear,

    Is the torch pictured supose to have the cv0076 part?
    Mine does and is chiped, Can I run with out it?


    It looks like this one:
    http://www.ebay.com/itm/281006865866...84.m1438.l2649

  19. #19

    Default

    Yes yours is supposed to have it, if it is an s 75 and yes you need it.
    It insulates the torch head and protects it. Why kind of "chip" do you have?

    The A81 pictured above is different and does not use one.

  20. #20

    Default

    Last edited by Gman; 04-15-2013 at 07:32 PM. Reason: resize pic

Similar Threads

  1. Power Pro 205 -- Plasma Question
    By scootarida1 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 15
    Last Post: 12-28-2012, 06:15 PM
  2. Another plasma cutter question.
    By Brian Ski in forum Everlast Plasma Cutters (PAC)
    Replies: 20
    Last Post: 04-18-2012, 05:55 AM
  3. Power Plasma 50 Question
    By morgaj1 in forum Everlast Plasma Cutters (PAC)
    Replies: 1
    Last Post: 06-11-2011, 01:59 AM
  4. PP 256 plasma function question
    By Wrenchtamer in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 6
    Last Post: 08-03-2010, 03:48 PM
  5. Question about 2 pin connector on the Power Plasma
    By I_Love_Plasma in forum Everlast Plasma Cutters (PAC)
    Replies: 2
    Last Post: 03-13-2010, 11:45 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •