Share
Results 1 to 4 of 4

Thread: Giving the 200DX a workout tonight.

  1. #1

    Default Giving the 200DX a workout tonight.

    I'm welding a charge cooler for my turbo bike.

    Note, when welding at 150 amps on an aircooled torch for a while, don't inadvertently bump the gas lens cup into a mounting tab. Kind of made it crack.
    Had to finally replace cup after two years of use.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  2. #2

    Default

    150 amps seems like alot. How thick is the aluminum ?
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #3

    Default

    I am welding the end tanks onto the core. The core is a bit difficult to heat up and it is relatively massive on the edges. ~ .375" square or so on each edge.

    It is realistically closer to 120-130 amps after the weld gets going, but it is higher in the beginning.

    It's basically one of these:

    Click image for larger version. 

Name:	intercooler.jpg 
Views:	299 
Size:	17.8 KB 
ID:	9885

    The welds are between the corners and formed / welded end caps made from .100-.125" thick sheetmetal.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  4. #4

    Default

    Show us some pics when you're done please.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

Similar Threads

  1. Buy the Powertig 200dx or save for The Dynasty 200dx
    By AfroPaul in forum TIG Welding (GTAW/GTAW-P)
    Replies: 40
    Last Post: 05-13-2013, 07:18 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •