Share
Results 1 to 5 of 5

Thread: Almost NOOB, getting ready to order a 200DX

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default Almost NOOB, getting ready to order a 200DX

    Well, I'll be moving and of April, and finally have a shop again.
    I'm looking into making custom bike frames, I have some plans for a kiln (heat treating) and think I have a way to hydroform aluminum.
    Wish I could afford the 250EX, but realistically it'll probably be the 200DX, though I do plan to get a wp-20 style torch and build a water chiller.
    I've got the rad from an old (50's probably) 2 cylinder peter engine, it's about 18"x18"x3" and should dissipate enough heat even without a fan (though I'll probably add a slow one).

  2. #2

    Default

    You will love the Powertig 200DX ... GR8 machine!
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  3. #3

    Default

    I'll second Winky on that one. The Everlast 200DX is a really nice welder. Nice feature set and stable, reliable arc.

  4. #4
    Join Date
    Mar 2013
    Location
    North By God Carolina
    Posts
    44

    Default

    The 200DX is a great machine. I'm a fan of small torches so for most of my stuff it's an air cooled WP-9 (.120 wall DOM (Chopper frames)
    and the lightest whip I can find. Always hated big bulky torches.
    No Crack Too Tight, No Gap Too Wide. If You Don't Like The Way I Do It, I'll Let You Try It!

  5. Default

    Well, my name is down for when they come in stock.
    Going to use the stock torch for now, had to tighten my budget.

Similar Threads

  1. Ready to Buy a PowerTig 185
    By sportbike in forum Pre-sales, Sales and Shipping questions
    Replies: 7
    Last Post: 04-30-2013, 11:53 PM
  2. First 2013 200DX tested and ready to ship
    By Titan winch in forum Pre-sales, Sales and Shipping questions
    Replies: 2
    Last Post: 02-21-2013, 04:58 AM
  3. Boxing Day 200DX Pre-Order Sale
    By Titan winch in forum Pre-sales, Sales and Shipping questions
    Replies: 8
    Last Post: 01-05-2013, 03:35 AM
  4. Think I might order my 200DX this week
    By Winky in forum Pre-sales, Sales and Shipping questions
    Replies: 34
    Last Post: 06-03-2012, 01:57 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •