Share
Results 1 to 16 of 16

Thread: HF works, but Arc wont start !!!

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default

    My issue was on 2t, 2sec. pre flow, dc, 55-60 volts, no foot pedal.

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Gman View Post
    My issue was on 2t, 2sec. pre flow, dc, 55-60 volts, no foot pedal.
    2 seconds is a long preflow time. You are aware that the arc will not even try to start for two seconds from when you push the switch? The HF should be able to jump a gap of at least .125-.250". If it doesn't transfer to the main arc, check for possible ground issues. One person had the ground wire come out inside the rubber boot at the plug.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    I've had the preflow all over the place. The 2 seconds is a +/-.
    Yes, I can hold it 1/2" away and still get spark.
    I'll have to check that.

Similar Threads

  1. PowerPro 256 makes HF but wont start arc
    By acannell in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 5
    Last Post: 06-25-2016, 07:03 AM
  2. PP50 wont make second cut with out first turning machine off and on
    By xtreme cartz in forum Everlast Plasma Cutters (PAC)
    Replies: 33
    Last Post: 01-31-2013, 04:48 PM
  3. Torch wont arc
    By Fomdiddle in forum Everlast Plasma Cutters (PAC)
    Replies: 10
    Last Post: 09-08-2011, 12:53 AM
  4. 250 ex arc wont start
    By johnson697 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 18
    Last Post: 05-26-2010, 04:40 AM