    Ironically I am having the same issue with my PP50, but only when I am at the 50 amp setting after about 10 seconds of cutting.

    Air PSI is 75+, good ground, 5/8 mild steel 1/16 to 1/8 standoff. Not tripping the overload, and the problem goes away at 47 amps.

    3 water separators/filters, Motorguard air filter/dryer, inlet pressure regulated at 85psi running (pressure drop from 90+ when trigger is pulled).

    Not trying to hijack the thread, but it applies.
    Sticks
    Field Service Tech for a Concrete Paving Company
    Location: The corner of "No" and "Where"

    "If they break it, we will fix it"

    AKA

    "Find some scrap and build a new one"

  2. #2

    Default

    Quote Originally Posted by sticks View Post
    Ironically I am having the same issue with my PP50, but only when I am at the 50 amp setting after about 10 seconds of cutting.

    Air PSI is 75+, good ground, 5/8 mild steel 1/16 to 1/8 standoff. Not tripping the overload, and the problem goes away at 47 amps.

    3 water separators/filters, Motorguard air filter/dryer, inlet pressure regulated at 85psi running (pressure drop from 90+ when trigger is pulled).

    Not trying to hijack the thread, but it applies.
    It sort of applies to this thread, but would have been better to start a new one as the PP60 and the PP50 use different torches. I run my PP50 about 65PSI and my PP60 I run at 72. Sounds like you have dry air, good flow, good ground. So I would experiment with the air pressure. Make sure consumables are good as well.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  3. #3
    Join Date
    Feb 2013
    Location
    Corner of "No" and "Where"
    Posts
    46

    Default

    Quote Originally Posted by everlastsupport View Post
    It sort of applies to this thread, but would have been better to start a new one as the PP60 and the PP50 use different torches. I run my PP50 about 65PSI and my PP60 I run at 72. Sounds like you have dry air, good flow, good ground. So I would experiment with the air pressure. Make sure consumables are good as well.

    Will do. More air pressure for higher amps, or lower? Example - 20 amps - 65psi and 50 amps 70psi (more amps/more PSI)
    Sticks
    Field Service Tech for a Concrete Paving Company
    Location: The corner of "No" and "Where"

    "If they break it, we will fix it"

    AKA

    "Find some scrap and build a new one"

  4. #4

    Default

    Actually, lowering the air pressure isn't the best idea for cutting. It can be done, but I have found that there is a better way and you will get better results... Downsizethe consumables for the amperage is a better way. The air pressure you cited is too much on the input side and on the operating side. You should be at 90 psi NO more on supply while static. Operating you should be no more than 73 or so (officially). You can buy smaller diameter holes for the PowerPlasma torch. The S-25 consumables will fit the S-45 and are designed for low amp cutting at the same air pressure.

    Is the arc stuttering or going on and off completely?
    Last edited by performance; 04-06-2013 at 01:58 PM.

  5. #5
    Join Date
    Feb 2013
    Location
    Corner of "No" and "Where"
    Posts
    46

    Default

    Quote Originally Posted by performance View Post
    Actually, lowering the air pressure isn't the best idea for cutting. It can be done, but I have found that there is a better way and you will get better results... Downsizethe consumables for the amperage is a better way. The air pressure you cited is too much on the input side and on the operating side. You should be at 90 psi NO more on supply while static. Operating you should be no more than 73 or so (officially). You can buy smaller diameter holes for the PowerPlasma torch. The S-25 consumables will fit the S-45 and are designed for low amp cutting at the same air pressure.

    Is the arc stuttering or going on and off completely?
    On and off completely.

    And like a fool, I bought the 75pc consumable kit which are all the same size tips, #8 if I had to guess. I wish you guys had a variety pack of the 6, 8, and 10s.

    I'll adjust the inlet pressure to 90, and verify my operating pressure at the torch is 73ish. When it acts up again, I'll tinker with the air pressure up and down to see if it goes away.
    Sticks
    Field Service Tech for a Concrete Paving Company
    Location: The corner of "No" and "Where"

    "If they break it, we will fix it"

    AKA

    "Find some scrap and build a new one"

  6. #6

    Default

    My pp60s is at it again. Pulsing. Off and on. 73 psi. What gives? Any ideas?

  7. #7

    Default

    What torch do you have? Does it pulse with just firing the pilot arc?

    I swapped consumables yesterday and had the same problem, in my case, I knew the air was dry and PSI was fine. Turned out, the new electrode was bad (maybe I did not get it tight). Swapped it and finished the job. Look at the electrode, make sure there are not burns on it.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. Using your portable mig as a simple wire feeder w/gas powered welder - 100% dty cyl
    By sticks in forum Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
    Replies: 5
    Last Post: 11-04-2013, 12:11 PM
  2. Power Plasma 50 plasma cutter....
    By CGCINC in forum Customer Testimonials
    Replies: 4
    Last Post: 07-20-2012, 12:58 PM
  3. Need to plasma cut some circles/holes soon. Cheap magnetic circle plasma jig.
    By everlastsupport in forum Personal Projects (no welder required)
    Replies: 5
    Last Post: 05-15-2012, 03:06 AM
  4. Dad'sMONSTER flathead V8 powered welder
    By Mikeymetal in forum Heavy Equipment and Commercial Projects
    Replies: 23
    Last Post: 10-13-2011, 03:53 PM
  5. Powered Bead Roller/Flanger
    By worntorn in forum Other Custom Fabrications
    Replies: 10
    Last Post: 04-17-2011, 01:11 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •