    I'm having a toss up between the 185 and the 200, yes I know, they have been threads about this, i read them .
    my toss up is, i'll be new to welding. my budget allows me to get a dual voltage 185 which is very convenient. I can sacrifice and get the 200DX by sacrificing the dual voltage feature and just get the 240v model. I'm probably never go over 1/4" since my goal is just auto fabrication, stainless and aluminum piping etc.
    The 200DX has the pulse feature, which I don't know if i'll use or have to.
    So to those who had this toss up, which would you choose. I guess this comes down to convenience of dual voltage vs Pulse feature that i may not use.
    is there anything the 185 is possibly better at welding wise. I'll also have to get a pedal for the 185, so that more $$

  2. #2

    Default

    I have owned both machines, upgraded to the 200DX for the extra options and pulse. The 2013 185 is priced on Ebay $1020 with free pedal , no stick holder . The 200DX 2012 model with pulse on Amazon $1026.00 pedal, torch , stick holder ground cable ect.

    Your choice .

    Mark might know the difference in machine options.
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  3. #3
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by cbmkr View Post
    I have owned both machines, upgraded to the 200DX for the extra options and pulse. The 2013 185 is priced on Ebay $1020 with free pedal , no stick holder . The 200DX 2012 model with pulse on Amazon $1026.00 pedal, torch , stick holder ground cable ect.

    Your choice .

    Mark might know the difference in machine options.
    With Amazon you can't always go by the picture. They may be 2012 or 2013 models as they are really bad about changing the pictures.
    Long arc, short arc, heliarc and in-the-dark!

  4. #4

    Default

    I'd go with the 200dx, it's better to have it and not need it than to need it and not have it.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  5. Default

    Quote Originally Posted by zoama585 View Post
    I'd go with the 200dx, it's better to have it and not need it than to need it and not have it.
    I agree with zoama. I had a Hobart mig welder, then a Hobart 165i, out grew them both in a few projects, went for the pp256. I haven't been above 150 on this machine yet, but I have a 1/4 aluminum project coming up and ill make some money on it, Im happy not to be turning it away.
    "The notorious forum spamming troll."

  6. #6
    Join Date
    Mar 2013
    Location
    North By God Carolina
    Posts
    44

    Default

    Pulse, I just got done with a little buildup job on some aluminum for a local machinist.
    So for ####s and grins I turned the pulse on and I was impressed with how easy it is
    to do buildup with it on. Especially near the edges. Pulse is worth the few extra duckets.

    The 200DX is a stud!
    No Crack Too Tight, No Gap Too Wide. If You Don't Like The Way I Do It, I'll Let You Try It!

  7. #7

    Default

    Do you have 30 amp 240v accessible where you will be using the welder?

    Welding 1/4" with the 185 will be really pushing it.

    I have a 2 year old 200dx and use it for pretty much what you are intending to use it for.
    I am also heavily looking at a 185 to put in my trailer to have on hand at the track for those "oh ####, if only I had a welder I wouldn;t have to load up and go home" times.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  8. Default

    thanks for the input, yes I have access to 240v in my garage. The amperage part i'm not sure of, it's the plug for my dryer.

  9. #9
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by SoFlaZ06 View Post
    thanks for the input, yes I have access to 240v in my garage. The amperage part i'm not sure of, it's the plug for my dryer.
    Dryer plugs are typically 30 amps.
    Long arc, short arc, heliarc and in-the-dark!

  10. #10

    Default

    Quote Originally Posted by SoFlaZ06 View Post
    thanks for the input, yes I have access to 240v in my garage. The amperage part i'm not sure of, it's the plug for my dryer.
    You shoudl be good to go with a 200dx. I use mine with a 100+ ft 10awg extension cord from a 240V dryer outlet.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  11. Default

    Quote Originally Posted by SoFlaZ06 View Post
    I'm having a toss up between the 185 and the 200, yes I know, they have been threads about this, i read them .
    my toss up is, i'll be new to welding. my budget allows me to get a dual voltage 185 which is very convenient. I can sacrifice and get the 200DX by sacrificing the dual voltage feature and just get the 240v model. I'm probably never go over 1/4" since my goal is just auto fabrication, stainless and aluminum piping etc.
    The 200DX has the pulse feature, which I don't know if i'll use or have to.
    So to those who had this toss up, which would you choose. I guess this comes down to convenience of dual voltage vs Pulse feature that i may not use.
    is there anything the 185 is possibly better at welding wise. I'll also have to get a pedal for the 185, so that more $$
    You don't have to sacrifice the dual voltage. The Canadians sell the 200DX-D. CAD $1300.

    http://www.everlastwelders.ca/tig-we...g-200-dx-d.php

    rivets

  12. #12
    Join Date
    Mar 2013
    Location
    North By God Carolina
    Posts
    44

    Default

    Hey guys, I just bought a new 200DX and to me it's a clone of the Miller Dynasty performance-wise. I love this thing!

  13. #13

    Default

    No, not a clone. I think the arc is actually better than the 200 Dynasty...and the duty cycle doesn't begin to compare.

    The prices you are quoting sounds high I think. Give me a call, and I can work on a better price for you.

  14. #14
    Join Date
    Sep 2011
    Location
    Middleburg Florida
    Posts
    556

    Default

    Pulse... one of those things you'll almost never use, until it makes a job so much easier. I was patching a Y pipe for a Peterbilt exhaust last night. Old one had rusted through in a number of spots, owner had to be back on the road today, new part was several hundred bucks and at least a day or two out. Cleaned for near 2 hours, and still wasn't happy with it, but it had to be done. Laid in some patches, got them fit up and tacked the hell out of them. Everything was going ok till I hit the thinnest area, rusted from 16ga probably down to half that. Holes liked to appear from what seemed like solid metal and I got weary of chasing them. Bring in the pulse. Set it to 3's, made it through the worst area with relative ease.

    That's the second or third time I've used it since last summer when I got my 200DX and it was worth every minute of waiting for that model and every penny I spent on that feature. I know it saved me at least 2-3 dozen four letter words last night
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

  15. Default

    Quote Originally Posted by performance View Post
    No, not a clone. I think the arc is actually better than the 200 Dynasty...and the duty cycle doesn't begin to compare.

    The prices you are quoting sounds high I think. Give me a call, and I can work on a better price for you.
    why did you call it a 200DX?

  16. #16

    Default

    We had the 250EX and a 200 lx before we had the 200 DX. Truth be known, we took a cue from the auto industry. DX is the base model with the lx the better and the EX the top of the line. The 200 DX was coincidental more than anything. I guess we're responsible for Longevity copying our nomenclature (but not understanding what it means). The "T" is added to any TIG product to denote digital. So if we were to bring out a digital 200dx, it would be a 200 dxt.

  17. #17
    Join Date
    Mar 2013
    Location
    North By God Carolina
    Posts
    44

    Default

    The only thing I'd change on mine is the plastic shield over the controls.
    It would be much better IMHO if it opened down instead of up. Or, if you
    could just remove it all together!

  18. Default

    Thanks for all the replies, 240v 200dx it is :thumbup:

  19. Default

    Wise choice. You won't be disappointed. I went with the 200DX, initially was thinking the 185. I do believe the 200 is their most stable unit.
    Everlast PowerTig 200DX
    Miller 120 Mig

  20. #20
    Join Date
    Sep 2011
    Location
    Middleburg Florida
    Posts
    556

    Default

    Quote Originally Posted by willida View Post
    Wise choice. You won't be disappointed. I went with the 200DX, initially was thinking the 185. I do believe the 200 is their most stable unit.
    Indeed. I was originally worried I'd miss something for not going with the 250EX or 225LX, but I've yet to run it to max capacity, and I haven't found myself looking for any of the 'missing' features. I'd buy one again in a heartbeat.
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

Similar Threads

  1. PowerTig 200dx question
    By AnimalMother in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 02-25-2016, 01:44 AM
  2. PowerTIG 200DX
    By Sparky_Mark in forum Pre-sales, Sales and Shipping questions
    Replies: 4
    Last Post: 10-18-2015, 04:09 AM
  3. PowerTig 200DX Stuck in AC - help!
    By silverbullet in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 07-12-2013, 11:11 AM
  4. Buy the Powertig 200dx or save for The Dynasty 200dx
    By AfroPaul in forum TIG Welding (GTAW/GTAW-P)
    Replies: 40
    Last Post: 05-13-2013, 07:18 PM
  5. Thinking about a PowerTig 200DX
    By Winky in forum General Welder Questions
    Replies: 5
    Last Post: 05-06-2012, 02:06 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •