Hey, welcome back, haven't heard from you in a while.
What's your budget? :-) And what's your tolerance? I'm sure someone will come back with a mag drill suggestion... And there's Petrogen.com, a cutting system that uses gasoline instead of acetylene. The videos at their site are offline today, but cool to watch.
Why is the plate soaking off the heat so fast?