  1. #7
    Join Date
    Feb 2013
    Location
    Corner of "No" and "Where"
    Posts
    46

    Default

    I'm coming in late to this, but if you are still fighting this, I'd spend the $40 on a Champion CT7 plug cutting drill bit. 1" max depth so you would have to probably end up coming up from the bottom, twist drill bit, or use a torch for the last 3/8". Don't need a mag drill, just a good 1/2" hand drill.

    Crane mounting holes...you really want to have tight tolerance on those bolt holes unless this is only like a #3k crane.

    ETA - I have done multiple layers of oxy cutting. It is a PITA, but if you have a drilled pilot hole that helps. Your top hole will be 3/4 but you will be closer to guesswork on the bottom of the hole due to the nature of the torch flame drift, angle of the torch head...just going to be ugly in general. Not helping that you are doing the 1" first then the 3/8".
    Last edited by sticks; 03-24-2013 at 11:23 AM.
    Sticks
    Field Service Tech for a Concrete Paving Company
    Location: The corner of "No" and "Where"

    "If they break it, we will fix it"

    AKA

    "Find some scrap and build a new one"

Similar Threads

  1. Everlast Super200P died. Performed "diode-ectomy". Now it's welding again!
    By jakeru in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 18
    Last Post: 01-27-2015, 10:24 PM
  2. Northern Industrial 1644910 AD Helmet Opinions? (3.82" x 2.44" view area)
    By Welderooni in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 01-10-2013, 04:49 PM
  3. Replies: 11
    Last Post: 10-30-2012, 07:43 PM
  4. Cutting 3"x3"x3/16" Angle
    By NRM in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 7
    Last Post: 07-02-2011, 12:56 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •