  1. Default new 250EX/HW20 handpiece

    I just got my 2013 250EX . I had a Miller syncrowave 250 which I loved but in my work weld a lot of thin stainless and have been having trouble with excess heat/distortion so bought the 250EX mainly for the pulser. I didn't much like the supplied handpiece and wanted to use my ESAB HW-20 handpiece as I have lots of gas lens, etc. from .040" to .125". I didn't want to shell out three hundred bucks like this guy :

    http://www.everlastgenerators.com/fo...tos-and-Part-s

    So I made my own adapter to use what I had. I robbed the switch out of the supplied handpiece and zip tied it to the HW-20. I have a Barnard water cooler so used it as well. The 250 EX seems to work great (after I set the point gap from about .075" to .032").Click image for larger version. 

Name:	tig1.jpg 
Views:	362 
Size:	90.7 KB 
ID:	9805Click image for larger version. 

Name:	tig2.jpg 
Views:	358 
Size:	87.8 KB 
ID:	9806Click image for larger version. 

Name:	tig3.jpg 
Views:	345 
Size:	92.3 KB 
ID:	9807

  2. #2
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Gotta admire a clever workaround. Welcome to the forums, Marvin!
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  3. #3
    Join Date
    Mar 2011
    Location
    mission viejo CA
    Posts
    92

    Default

    did you machine up that dinse adapter to lug ??
    if not where did you source it ?
    Lincoln precision tig 275
    Miller Syncrowave 350 Tig
    Miller 250 Mig
    old miller 200 Mig
    HF 151 Mig
    HF 100 FC
    Victor Journeyman Oxy/Ace set up
    Bunch of tools of the trade to much to list

  4. #4

    Default

    Welcome aboard Marvin,

    I have the same cooler. It's a beast (almost as loud as the welder). Nice mod on the welder and torch. CKs are expensive, but the super flex hoses are nice.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  5. Default

    Quote Originally Posted by Wookie View Post
    did you machine up that dinse adapter to lug ??
    if not where did you source it ?
    I couldn't find one so I machined it up myself. BTW, it works great, love the 250EX!