Share
Page 1 of 2 12 LastLast
Results 1 to 20 of 24

Thread: my PowerPro 256S (2013)

  1. Default my PowerPro 256S (2013)

    I received my pp256s today.

    here are a few starter pics:

    L>R
    a- Front new design for 2013
    b- close up of the front panel
    c- front panel connections
    d- rear panel

    note: I was surprised this came with a molded 6-50P installed on the power cord.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	pp256_front.jpg 
Views:	618 
Size:	146.0 KB 
ID:	9689   Click image for larger version. 

Name:	pp256_front panel.jpg 
Views:	669 
Size:	141.4 KB 
ID:	9688   Click image for larger version. 

Name:	pp256_front_connectors.jpg 
Views:	535 
Size:	143.7 KB 
ID:	9687   Click image for larger version. 

Name:	pp256_back_panel.jpg 
Views:	567 
Size:	147.8 KB 
ID:	9686  
    Last edited by halojumper; 03-06-2013 at 02:57 AM.

  2. #2

    Default

    Nice, post some pics when you get a chance to weld with it. I had the old PP256 and thought it was nice machine. I really like the newer look that they have.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  3. #3

    Default

    Looks really nice. Could you post height/width/length dimensions and weight? Thanks!
    Everlast PowerArc 140ST

  4. Default

    I will post more info when I get the chance

    I started an autocad file I will share when thats done, as well as the basic measurements.

    hopefully I can create some heat with it this weekend.



    I made a .pdf of the included operation instructions if anyone wants a copy, just ask and provide an email

    it's too big to host here (it's 700k)

  5. Default

    Click image for larger version. 

Name:	pp256_box as received.jpg 
Views:	543 
Size:	136.4 KB 
ID:	9713 Box as received from UPS. luckily it was fairly well strapped, hate to have seen it w/o 'em

    Click image for larger version. 

Name:	pp256_heavy package.jpg 
Views:	978 
Size:	146.6 KB 
ID:	9712 Box is heavy. 85 lbs according to UPS

    Click image for larger version. 

Name:	pp256_packaging.jpg 
Views:	540 
Size:	146.0 KB 
ID:	9711 opening the box for the first time (there is a double layer cardboard on top)

    Click image for larger version. 

Name:	pp256_accessories_box.jpg 
Views:	548 
Size:	141.9 KB 
ID:	9710 the accessories box as received

    Click image for larger version. 

Name:	pp256_power_plug.jpg 
Views:	557 
Size:	145.7 KB 
ID:	9709 the pre-terminated power plug

    Click image for larger version. 

Name:	pp256_bagged.jpg 
Views:	560 
Size:	143.5 KB 
ID:	9708 fresh out of the box

    Click image for larger version. 

Name:	pp256_data_placard.jpg 
Views:	624 
Size:	140.7 KB 
ID:	9707 data placard and unit serial number on the side of the unit

    Click image for larger version. 

Name:	pp256_accessory_box_contents.jpg 
Views:	686 
Size:	143.7 KB 
ID:	9706 accessories removed from the box

    more pics / info to follow later....

  6. Default

    here are some basic drawings with the basic dimensions

    more detailed drawings will become available as I find the time to make 'em

    I used a tape measure, consider measurements to be +/- 1/16"

    on the front, the gas outlet and pilot arc post do stick out a little bit as well as the
    gas inlet and power cord on the back. these measurements should suffice for finding or making a cart
    for this thing to fit on.
    Attached Files Attached Files

  7. #7

    Default

    These units have new regulators for tig.

  8. Default

    Click image for larger version. 

Name:	pp256_foot_control.jpg 
Views:	563 
Size:	144.0 KB 
ID:	9728
    foot control

    Click image for larger version. 

Name:	pp256_foot_control_connector.jpg 
Views:	532 
Size:	146.2 KB 
ID:	9727
    foot control connector

    Click image for larger version. 

Name:	pp256_foot_control_front.jpg 
Views:	559 
Size:	147.0 KB 
ID:	9726
    foot control front side (note: no knob to fiddle with)

    Click image for larger version. 

Name:	pp256_SR18_torch.jpg 
Views:	552 
Size:	145.3 KB 
ID:	9725
    SR-18 Torch as received

    Click image for larger version. 

Name:	pp256_SR18_torch_lable.jpg 
Views:	556 
Size:	145.3 KB 
ID:	9724
    SR-18 torch parts tag

    Click image for larger version. 

Name:	pp256_SR18_torch_b.jpg 
Views:	555 
Size:	146.6 KB 
ID:	9723
    SR-18 torch


    Click image for larger version. 

Name:	pp256_SR18_torch_parts.jpg 
Views:	543 
Size:	147.4 KB 
ID:	9722
    SR-18 Torch parts

    Click image for larger version. 

Name:	pp256_SR18_torch_head.jpg 
Views:	551 
Size:	147.8 KB 
ID:	9721
    SR-18 torch head

    Click image for larger version. 

Name:	pp256_SR18_torch_connectors.jpg 
Views:	535 
Size:	147.3 KB 
ID:	9720
    Torch connections

    Click image for larger version. 

Name:	pp256_bagged_hardware.jpg 
Views:	540 
Size:	146.8 KB 
ID:	9729
    supplied bagged hardware


    More coming. If you want to see anything specific or ask questions, please do.

  9. Default

    Click image for larger version. 

Name:	pp256_ground_clamp.jpg 
Views:	551 
Size:	146.2 KB 
ID:	9738
    Click image for larger version. 

Name:	pp256_ground_clamp_closeup.jpg 
Views:	718 
Size:	147.6 KB 
ID:	9737
    Ground Clamp

    Click image for larger version. 

Name:	pp256_rod_holder.jpg 
Views:	546 
Size:	145.9 KB 
ID:	9736
    Rod holder

    Click image for larger version. 

Name:	pp256_argon_reg.jpg 
Views:	554 
Size:	146.6 KB 
ID:	9735
    Click image for larger version. 

Name:	pp256_argon_reg_closeup.jpg 
Views:	526 
Size:	146.6 KB 
ID:	9734
    Argon Reg/flow meter

    Click image for larger version. 

Name:	pp256_air_regulator.jpg 
Views:	526 
Size:	146.8 KB 
ID:	9733
    Click image for larger version. 

Name:	pp256_air_regulator_closeup.jpg 
Views:	539 
Size:	137.1 KB 
ID:	9732
    Air Reg/filter

    Click image for larger version. 

Name:	pp256_S75_plasma_torch_closeup.jpg 
Views:	530 
Size:	146.6 KB 
ID:	9739
    S75 Plasma Torch

    Click image for larger version. 

Name:	pp256_plasma_airflow_gauge.jpg 
Views:	555 
Size:	145.4 KB 
ID:	9731
    Plasma Torch flow meter (I think)

    Click image for larger version. 

Name:	pp256_airhose.jpg 
Views:	532 
Size:	146.1 KB 
ID:	9730
    supplied air hose

  10. #10

    Default

    Congratulations on your new PP256S! A word of caution, on my 2012 PP256 the supplied screws to install the Plasma air regulator at the rear of my unit were TOO long and came into contact with the windings on the transformer just inside the case at that location. I just reduced the length of the one screw that was too close and was in conflict with the transformer. You unit may not have this issue. Enjoy!!
    Everlast PowerPro 256
    Everlast W300 Cooler
    Everlast Cart 250

    Millermatic 211
    Spoolgun 100
    Miller HD Cart

    Victor 315 Torch sitting on a Harper 830-86 cart

  11. Default

    Quote Originally Posted by performance View Post
    These units have new regulators for tig.
    The Argon regulator, as shown above (pics)

    Box has a part number: AR GH-191

    this specific part number is not in the manual that comes with it, but in the manual, all
    the different part numbers that are listed, have the same specifications.

    The pressure gauge scale reads in PSI (red, inner numbers(0-4000) and kg/cm² (black, outer numbers (0-280)

    the flow meter has two scales;

    Ar 0-25 L/min 20°C 0.35MPa

    CO2 0-25 L/min 20°C 0.35MPa

  12. Default

    Quote Originally Posted by Grandslam99 View Post
    Congratulations on your new PP256S! A word of caution, on my 2012 PP256 the supplied screws to install the Plasma air regulator at the rear of my unit were TOO long and came into contact with the windings on the transformer just inside the case at that location. I just reduced the length of the one screw that was too close and was in conflict with the transformer. You unit may not have this issue. Enjoy!!

    thanks for the heads up!

    due to your advice and others having issue with the HF gap, I decided to pull the cover off my unit and take a peek, just to make sure everything was okay.

    sure enough, the same clearance problem exists with the air regulator mount as last year (surely someone at Everlast knew about this?????)

    they could move both holes down about 1.5cm and be okay (or maybe move the transformer forward some?)
    the quickest fix would be to supply 2 shorter screws.


    Click image for larger version. 

Name:	pp256_air_reg_mount_problem-a.jpg 
Views:	811 
Size:	146.4 KB 
ID:	9789

    Click image for larger version. 

Name:	pp256_air_reg_mount_problem-b.jpg 
Views:	792 
Size:	134.7 KB 
ID:	9790

    Click image for larger version. 

Name:	pp256_air_reg_mount_problem-c.jpg 
Views:	787 
Size:	139.7 KB 
ID:	9791



    The HF gap is new and improved quite a bit from what I've seen in other pictures... this one shouldn't move at all
    (located on the left side, front)

    Click image for larger version. 

Name:	pp256_HF_gap.jpg 
Views:	898 
Size:	143.5 KB 
ID:	9792

    Click image for larger version. 

Name:	pp256_HF_gap_closeup.jpg 
Views:	891 
Size:	144.4 KB 
ID:	9793

  13. #13

    Default

    Can that be retrofitted into an older model? I like that much better.
    My Stuff:
    Everlast PP256
    Century Mig 135
    BladeRunner Inverted Jig Saw
    HF 14" Chop Saw
    Box full of HF 4" Angle Grinders
    Home made tank roller!

  14. Default

    Quote Originally Posted by Ron66 View Post
    Can that be retrofitted into an older model? I like that much better.
    That would be great if you can get the part.
    I have tried a number of times (more than one PM), with no luck.
    I would be happy to purchase the new points, and retrofit myself.

    How about it Oleg?

    Thanks,
    rivets

  15. #15
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    From the looks of it, you would change the whole HF board. Probably not worth it unless you slam your welder around all the time like a mobile welding truck. The points on an inverter get so little on time, that even the old style should last a lifetime.


    Quote Originally Posted by Ron66 View Post
    Can that be retrofitted into an older model? I like that much better.
    Long arc, short arc, heliarc and in-the-dark!

  16. #16

    Default

    I have had to re gap before. If you exercise the hf start to much, like when you weld something that you can't get a good torch position, the points move probably from too much heat.
    My Stuff:
    Everlast PP256
    Century Mig 135
    BladeRunner Inverted Jig Saw
    HF 14" Chop Saw
    Box full of HF 4" Angle Grinders
    Home made tank roller!

  17. Default

    Hello,

    I bought this unit in April and since I got this grate machine I have always wondered if the fans ever shut off, its so loud, are they really ment to run at idle on power up?

    Thanks

    Richard

  18. #18

    Default

    Yes. They are supposed to be running constantly. The noise is relatively small compared to welding or many activities that go on in the shop. The fan provides the duty cycle of the unit. On demand fan units operate at lower duty cycles as well.

  19. Default

    Thank you for the quick reply, and you are right the fans are quickly drowned out when I get to work.

  20. Default

    My Miller cooler, with it's bronze gear-pump, drowns out Everything in my shop!

    Also I love the gauge in the front of the machine, I TyeRap my extended gauge to the front in my older version...

Similar Threads

  1. Powerpro 256s not cutting
    By Bluediemond in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 6
    Last Post: 01-03-2015, 08:31 PM
  2. Powerpro 256s shipping date
    By jpmitch in forum Pre-sales, Sales and Shipping questions
    Replies: 5
    Last Post: 12-05-2013, 10:05 PM
  3. Why is my PowerPro 256S Pulse lower than spec, am i miss reading it?
    By schric11 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 1
    Last Post: 12-02-2013, 08:26 PM
  4. Thanks Oleg, for the 2013 PowerPro 256s
    By Big Paulie in forum Customer Testimonials
    Replies: 5
    Last Post: 04-30-2013, 10:50 PM
  5. 2013 PowerPro 205S
    By bluetec in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 8
    Last Post: 03-14-2013, 01:18 AM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •