    Default -Colorful Stainless steel-

    I just started stainless today in class and think out of everything... TIG on stainless is my favorite. I love the colors! I think it would be cool if we had a tread of just cool colored welds? Here's a couple from today, one being a flat T and the other a Horizontal T. I'd love to see people's cool stainless stuff - RJ
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	IMG_7952.resized.jpg 
Views:	515 
Size:	46.6 KB 
ID:	9782   Click image for larger version. 

Name:	IMG_7953.resized.jpg 
Views:	467 
Size:	52.1 KB 
ID:	9783  

  2. #2
    Join Date
    Jan 2013
    Location
    Minneapolis, MN
    Posts
    80

    Default

    Just another...Click image for larger version. 

Name:	rj.jpg 
Views:	528 
Size:	144.1 KB 
ID:	9794

Similar Threads

  1. How do you polish / finish stainless steel?
    By DaveO in forum General Welding Questions
    Replies: 20
    Last Post: 09-13-2013, 04:09 PM
  2. Stainless Steel Android Guy
    By cpierce18 in forum Personal Projects (no welder required)
    Replies: 4
    Last Post: 03-26-2012, 03:21 PM
  3. Stainless Steel oxy-acetilene welding, how-to?
    By lwmar in forum General Welding Questions
    Replies: 7
    Last Post: 10-06-2011, 05:12 AM
  4. Stainless steel cup brushes
    By jdt1986 in forum General Welder Questions
    Replies: 7
    Last Post: 06-13-2011, 05:34 AM
  5. Stainless Steel Stick Welding?
    By Oxide00 in forum General Welding Questions
    Replies: 13
    Last Post: 04-27-2011, 02:31 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •