  1. #1
    Join Date
    Jan 2013
    Location
    Minneapolis, MN
    Posts
    80

    Default Micro TIG WELDING! Lets see em!

    Started laying down some small beads today, thought I would share some pictures of em'...a dime is placed for referanceClick image for larger version. 

Name:	IMG_7929.resized.jpg 
Views:	1336 
Size:	113.8 KB 
ID:	9579. I was right around 70amps. I'd love to see more of whats is out there - Ryan

  2. Default

    Nice bead there, Johnson. Cant wait to get my machine.
    Soon to be 2013 250EX tig machine
    Lincoln Idealarc DC250 with LN7 wire feeder
    RSG250 spool gun and controller for above.
    Hypertherm Powermax85 with Machine and hand torch
    Bridgeport Milling Machine w/DRO and Powerfeed
    South Bend 9 lathe WW2 vintage
    Devilbiss 6.5hp 80gal 175psi 2 stage compressor
    HF blast Cabinet modified for foot pedal operation better gun.
    Oxy/A torches
    Delta 4x6 band saw
    Hand and power tools up the wazoo.

    The name's "Marcel" in case I forget to sign.

  3. #3
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Very cool, nicely done. Are you experimenting with small beads or is that part of something else?
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  4. #4
    Join Date
    Jan 2013
    Location
    Minneapolis, MN
    Posts
    80

    Default

    My instructor kept telling me to scale it down... after some experimenting I welded that piece. I think he is trying to get us ready for stainless. My new machine will be here in a week or so and I can't wait to see how well it preforms against a dynasty 350. I know it's kinda unfair, but I have good hopes My Micro 185 had a really nice arc and I'm guessing the 250ex will be better. I'll be posting lots of shots of my welds from the 250ex

  5. #5
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    Hey, no fair! I don't have a Micro 185! Plus you really should be welding aluminum and showing off the A/C function of that machine anyways! Take advantage of that as some of us don't have fancy A/C and D/C welders!

    I have to say that I've done some decent beads on my PA 160 STH, even though it's a bare bones unit. I have yet to weld a test bead though...everything lately has been project stuff with short beads.

    I look forward to seeing more shots of your welds, especially with your new 250ex.
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  6. #6
    Join Date
    Sep 2011
    Location
    Middleburg Florida
    Posts
    556

    Default

    70 amps? How thick is the base metal?

    I was thinking of running some more blades this weekend, I like to play with them every couple weeks. Believe it or not, I find it a really good exercise to keep close control of the torch... yeah, you can practice on big stuff, but a bit of wiggle or varying arc length don't really show as easily as welding up .009 thick razor blades. I usually set the machine around 10A and pedal my way around.



    Bead is a bit tall, only had 1/16 filler on hand that day. Penetration is great, through and through. Bit of warping towards the end, I just set them on the table, no clamp or third hand (though I built some since then)
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

  7. #7
    Join Date
    Jan 2013
    Location
    Minneapolis, MN
    Posts
    80

    Default

    It was on 14 gauge......074" so 70 amps was on the lower end. The razor blade thing is great...gotta try that soon. And yes the Micro 185 WAS a good machine but sold it to help fund my 250ex. That should keep me busy for awhile I'll give the razors a go in a week when my new machine gets here.

  8. #8
    Join Date
    Sep 2011
    Location
    Middleburg Florida
    Posts
    556

    Default

    Quote Originally Posted by Johnson View Post
    It was on 14 gauge......074" so 70 amps was on the lower end. The razor blade thing is great...gotta try that soon. And yes the Micro 185 WAS a good machine but sold it to help fund my 250ex. That should keep me busy for awhile I'll give the razors a go in a week when my new machine gets here.
    Clean them well... the oil coating the blades infuriated me, couldn't feel it, couldn't see it till it made sparks and stink, but once I started rinsing in acetone, got much easier. I use 1/16 1.5% lanth sharpened 4+ length to thickness (more focus, less penetration) clean it with acetone too, clean your filler with acetone. I was using 1/16 309L on those, I'm going to use some.030 309L MIG wire I got in since then, next time.

    Got a nice thin one coming up this weekend or next, welding the ends of a rollpan into the rear bed of an S10. The body is like tinfoil on those, not going to be like the body work I used to do on pre 70's vehicles.
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

  9. #9
    Join Date
    Oct 2011
    Location
    Litchfield Park, AZ
    Posts
    370

    Default

    That looks good and good advice from your instructor. I have practiced some thinner material and it is not as easy to keep a small weld looking good as with thicker material.
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

  10. #10
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Don't know if I'd call it micro welding, but here are some fillet welds about .060" wide to secure some #10-32 nuts in place, without rolling over the edges or causing distortion to the threads.

    Click image for larger version. 

Name:	Nut5.jpg 
Views:	478 
Size:	78.2 KB 
ID:	9630 Click image for larger version. 

Name:	Nut3.jpg 
Views:	534 
Size:	53.5 KB 
ID:	9631
    Long arc, short arc, heliarc and in-the-dark!

  11. #11

    Default

    sweet....i have a 250 ex and is a very nice machine ,but i have been thinkin about getting a 255ext .
    250 ex
    205 mig
    milwaukee grinder
    140e mig

  12. #12

    Default

    Butt weld on 0.028" wall tubing. Not micro, but small for me!


    Some practice by Zanconato Custom Cycles, on Flickr


    Some practice by Zanconato Custom Cycles, on Flickr

  13. #13

    Default

    what kind of material is that zank?
    250 ex
    205 mig
    milwaukee grinder
    140e mig

  14. #14

    Default

    That's 410 stainless. 1.25" OD x 0.028" wall. I used 0.035" 309L filler. This is a fun drill because it really makes any change in bead width or travel direction pop out. And it's good practice for purging.

  15. #15
    Join Date
    Jan 2013
    Location
    Minneapolis, MN
    Posts
    80

    Default

    Another one!Click image for larger version. 

Name:	IMG_0391.resized.jpg 
Views:	464 
Size:	116.2 KB 
ID:	9652 about a 1/16th of an inch

  16. #16

    Default

    Heres one of some 22 ga parts i was fabbing for my car, the lead pencil tip is .045 dia. 25 amps dc

    Click image for larger version. 

Name:	micro weld.jpg 
Views:	580 
Size:	120.5 KB 
ID:	9675

    Best focus i could get with the camera that close
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  17. Default

    Quote Originally Posted by cbmkr View Post
    Heres one of some 22 ga parts i was fabbing for my car, the lead pencil tip is .045 dia. 25 amps dc

    Click image for larger version. 

Name:	micro weld.jpg 
Views:	580 
Size:	120.5 KB 
ID:	9675

    Best focus i could get with the camera that close
    Nice, Thats the kind of stuff that you just cant do with a mig.
    Soon to be 2013 250EX tig machine
    Lincoln Idealarc DC250 with LN7 wire feeder
    RSG250 spool gun and controller for above.
    Hypertherm Powermax85 with Machine and hand torch
    Bridgeport Milling Machine w/DRO and Powerfeed
    South Bend 9 lathe WW2 vintage
    Devilbiss 6.5hp 80gal 175psi 2 stage compressor
    HF blast Cabinet modified for foot pedal operation better gun.
    Oxy/A torches
    Delta 4x6 band saw
    Hand and power tools up the wazoo.

    The name's "Marcel" in case I forget to sign.

Similar Threads

  1. 22k or 47k for 2013 185 micro
    By joe n in forum Forum related Questions
    Replies: 1
    Last Post: 11-22-2013, 11:14 PM
  2. Micro TIG 185 $730
    By Johnson in forum Buy, Sale or Trade
    Replies: 1
    Last Post: 01-27-2013, 12:34 AM
  3. Power Tig 185 Micro Low Amp Use
    By cbmkr in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 09-27-2012, 01:27 AM
  4. 185 Micro HF?
    By Gtig in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 02-25-2012, 03:35 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •