    I brought my Imig 200 to work for my friend. All galvanized schedule 40 pipe 4" and 6", these are going to Texas just a few miles from the Mexico border. They will be going around well heads and barbed wire will be added to keep cows away from the well heads. I believe it's safe to call this over kill! I let some of the other welders try out my Imig 200, and they were all impressed. It's hard for some to believe a welder this small can put out this kind of heat! I believe their 220 outlet is on a 50 amp breaker.







    I welded these L's all day long today with my Imig 200.


    These are corner braces for the fence.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  2. #2

    Default

    Imig 200 .35 mig wire uphill weld.


    More uphill


    Uphill, moved a tick slow on this one.


    This was me on Wednesday.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  3. #3

    Default

    Material was ordered pre-cut


    Coped out with a plasma cutter


    I welded all day long with my Imig 200. I did stop to flip, move, fit, and help other people flip and move. I ran a complete 10lb spool of .35 wire through the welder today. I have ran more wire through larger welders in day, but I think for a dual voltage 200 amp welder a 10lb spool is impressive. I never bumped the duty cycle, but I did have some pauses throughout the day. Another welder gave my Imig a try and could not believe it! The welder performed solid all day long running on 220v 40 or 50 amp breaker.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  4. #4

    Default

    These frames are placed along the fence line, I can't remember how far apart they are set. I believe the barbed wire will be terminated on one side and attached/started to the other.


    All the frames will be set 3' deep in concrete, and inside the pipe will be filled with concrete. They do not want them to go anywhere! It's all a bit overkill for a barbed wire fence!
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  5. #5
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    That's quite a bit of pipe! It's really cool that you were able to use the Everlast MIG in an industrial type setting and it did what you "asked" it to do all day! What's better is the fact you might have converted some of the other guys there over to Everlast welders.

    My knees, back, and feet would NOT handle that abuse all day of kneeling down or standing up. I used to do that stuff at work for 8 hours a day (when I had to), but I think I'm getting softer, weaker, or just less tolerant. I know I'm certainly not getting any smarter! It's too bad you couldn't do some of the smaller assemblies (even just the "L"s) flat on a table so you could sit and give your knees a chance to rest.

    Great welds on that pipe! That's one heck of a barbed wire fence...but everything is bigger in Texas (or so they say).
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  6. #6

    Default

    I agree I bet some of the guys at the beginning were thinking "let's see how long this Chinese junk will make it" I bet by the end they were all impressed (even if they didn't admit it)... you know if it isn't red, blue, blah blah blah bull crap. Well they need to revise their list and add Everlast Green to it!
    Everlast PowerTig 200DX
    Everlast Supercut 50P
    I need a MIG.... which one to buy:
    I-Mig 160, I-Mig 200, or a MTS 160

  7. #7

    Default

    We run a IMIG-200 pretty hard as well, thinking about a second one. We do aluminum in a spool gun as well on hurricane shutters. FYI: 30amp breaker will run it for most jobs. We also use it on a 5500 watt porter cable generator and go mobile with flux-core wire. Great little machine. Just can not get rid of it do to size, power and mobile jobs.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  8. #8
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    Quote Originally Posted by everlastsupport View Post
    We run a IMIG-200 pretty hard as well, thinking about a second one. We do aluminum in a spool gun as well on hurricane shutters. FYI: 30amp breaker will run it for most jobs. We also use it on a 5500 watt porter cable generator and go mobile with flux-core wire. Great little machine. Just can not get rid of it do to size, power and mobile jobs.
    How thick of aluminum can you weld with the spool gun using your IMIG-200, Mike? I like that it runs off a 5500 watt genny for portability!
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  9. #9

    Default

    Based off a tig welder I would say 1/4" but that's a guess.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  10. #10
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    That's in the ballpark for what I was thinking too. All the other Spool guns that I've welded aluminum with in school were all 250 amps or more (and I don't remember machine settings from yesterday, let alone 10 years ago!).
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

Similar Threads

  1. This is a test post.
    By deevil in forum Introduce Yourself
    Replies: 1
    Last Post: 12-11-2015, 10:21 AM
  2. test
    By saravanan in forum Stick Welding (SMAW)
    Replies: 4
    Last Post: 05-22-2014, 01:28 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •