Share
Results 1 to 6 of 6

Thread: Making a wooden propeller....

Threaded View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default Making a wooden propeller....

    I posted this in the chat lounge but I wanted people to be able to find it in a search engine if they want to try it themselves so Im posting it here as well.

    I wanted a wood propeller but didn't want to pay for one so I decided to build one myself.
    I started out with 5 pieces of 1x8 @ 6' long and glued and clamped them overnight.

    Click image for larger version. 

Name:	IMAG2955_zpsc6cd60dc.jpg 
Views:	1806 
Size:	56.2 KB 
ID:	9511

    Then I made a mount to hold the propeller while working on it.
    I used 1" tubing with a bolt welded to it and a nut with handles welded to it. The mount was welded to an adjustable small welding table I made to slide in the rails of my welding table.

    Click image for larger version. 

Name:	IMAG2953_zpsa7dcef9b.jpg 
Views:	2122 
Size:	66.3 KB 
ID:	9512

    Then I drew out the propeller on the wood and put it on the mount to cut the bulk of the wood off to get the shape.
    I used a sawzall with a 12" blade to cut the rough shape.

    Click image for larger version. 

Name:	IMAG2974_zps4860a5f5.jpg 
Views:	2655 
Size:	56.7 KB 
ID:	9513




    Once I got it close with the sawzall.... I switched to a 4 1/2" grinder with some 60grit flap discs......you can't just tear into it, you need to "stroke" the wood so you don't gouge out huge valleys.





    After the flap disc, I went over it with 100 grit then 220 grit sandpaper.
    Then it is time to stain to color...



    Next I made a 3" nose cap. This looks nice but it is also how I hold the propeller to the wall mount.





    Last edited by CGCINC; 02-21-2013 at 10:50 PM.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

Similar Threads

  1. Making bedroom furniture...
    By CGCINC in forum Personal Projects (no welder required)
    Replies: 21
    Last Post: 10-14-2012, 11:35 AM
  2. Making new band saw tension bars
    By MigPlazArc in forum Other Custom Fabrications
    Replies: 1
    Last Post: 03-24-2012, 03:07 PM
  3. Project #1 (200 EXT Contest) by DVA: Jig for making BBQs
    By DVA in forum Other Custom Fabrications
    Replies: 0
    Last Post: 12-07-2011, 02:43 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •