    I'm sure I could just ask my instructor tues, but why wait. What's the shelf life on 6011, 6013 , and 7013's? Do they just stop welding good? what happens when they get old....any way to bring em back? Thanks

  2. Default

    I'd like to know as well. I'd like to have some around for 'just in case', but I know that some rods don't have an infinite shelf life, where as my mig/tig supplies should.
    (taking into consideration that where/ how you store them are important as well)

  3. #3

    Default

    How long will they last in storage,,,anywhere from a week to 25 years,,depending on who does the storing and how they do it,,,,there are no BBF dates on welding rods,,,paper rods like 6010,, 6011,, should be stored at room temp for many years and still work fine,,other rods need warmer temps if the package is opened and some can be reconstsituted at higher temps ,,,,information on how to store and recondition them is available..at different web sites..
    Some of those lies people tell about me, are true

  4. #4

    Default

    Today, I just used a 6013 I know are 15 years old, welded fine.
    They are kept in a air tight container.
    Moisture is bad.
    Power I-MIG-250P

  5. #5
    Join Date
    Jan 2013
    Location
    Minneapolis, MN
    Posts
    80

    Default

    Cool good to know! Thanks!

  6. #6
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Shelf life by the Military today its good, tomorrow through it out. Let’s see the welder is good to day if I take it off the shelf and use it but tomorrow it is scrap. It will not work its shelf life is up. Do not use it, it will not work warranty is up. But the one I took off the shelf yesterday is still good. That’s shelf life for the Military.
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  7. #7

    Default

    It depends on the type of electrode and how it's stored ... if you store 7018 in a cold wet environment it wont last long ... does OK if kept dry and electrode ovens are great ... I've used five year old 6013 that was stored in my house close to a heater register and it was fine.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  8. Default

    I have a 50# box of Airco 6013 and 6011 rods that I bought in 1978. They have been stored in a metal cabinet in my garage in Houston all these years. I pulled them out today to look at them, and they look like they did when I bought them. My loose rods don't look as good, but they still work fine, and they are all at least as old.

  9. Default

    An old trick with 6010. They will dry out in time, I grab a couple hands full lay them in the kitchen sink and run some water in the sink. Roll the rods around a bit. Take them back out to the shop and let them air dry for 2 to 3 days. Good as new!

Similar Threads

  1. PowerArc 200ST and 6010 Electrodes
    By Awelder in forum Stick Welding (SMAW)
    Replies: 3
    Last Post: 02-19-2018, 12:00 AM
  2. Electrodes for 255 EXT
    By oleblu72 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 12
    Last Post: 01-22-2018, 08:18 PM
  3. Stick Electrodes for use with PowerTig 200 DV?
    By MBfrontier in forum Stick Welding (SMAW)
    Replies: 8
    Last Post: 10-28-2014, 07:45 AM
  4. A81 long tips and electrodes
    By srp in forum Everlast Plasma Cutters (PAC)
    Replies: 2
    Last Post: 11-08-2013, 10:14 PM
  5. Anyone run cellulosic E6010 electrodes in TIG 210Ext?
    By Martine in forum Stick Welding (SMAW)
    Replies: 22
    Last Post: 12-09-2012, 09:19 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •