Thread: Found the limit of my mig

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default Found the limit of my mig

    I have a Century135 mig welder that I have owned for about 12 years now. It served me well but this weekend I had a pretty big job to do assembling some products I sell and welded for about 1.5 hours almost non-stop. Then I noticed that the arc and wire feed would just start to stop intermittently in the middle of a weld. I'm pretty sure I was hitting the dutycycle limit as this unit is only rated at 20%. If I waited about a minute in between 3/4" welds it was ok. Does this sound right? I never had this happen before. I expected if I ever hit the dutycycle limit it would just shut down.

  2. #2

    Default

    It does sound about right for a transformer machine. You may have done terminal damage to it. The fan should keep running to cool everything. Ours wills top welding, though the wire will continue to feed.

  3. #3

    Default

    You may want to give it a once over and clean the insides. It was likely overloading the welder, but at 12 years old, it likely has a bit of dust and dirt built up. Fan could be on its way out as well and not flowing enough air if the bearings are getting sketchy.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  4. #4

    Default

    I've thought that I was going to hit the duty cycle on my Imig 200 a few times when I was pushing hard to get a project done but I've not had the duty cycle light come on yet. Apparently this machine has a higher duty cycle than I do!
    IMig 200

  5. #5

    Default

    Yeah I was thinking about pulling it apart and giving it a good cleaning. Good thing to keep me out of trouble this weekend.

Similar Threads

  1. Found a great respirator
    By EmptyNester in forum General Welder Questions
    Replies: 6
    Last Post: 08-05-2012, 06:33 AM
  2. Everlast support, found this on eBay. Know anything about it?
    By 225 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 04-30-2012, 09:11 PM
  3. Need a generator and found this on EBAY....
    By CGCINC in forum General Welding Questions
    Replies: 15
    Last Post: 04-19-2012, 05:01 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •