    Default Project 3 from Rambozo. Category: General Welding Repair

    Someone backed a sprayer into a wall and broke off a rear mount. To be fair it was probably cracked for a while before that, from the looks of things.

    Click image for larger version. 

Name:	Toro 1.JPG 
Views:	853 
Size:	76.2 KB 
ID:	9380

    This time I did have 240V, so I finally got a chance to do some TIG with the 140ST and new torch control. Cut off some of the old mount point, and added a piece of angle to cover the hole and spread out the load a little. Used ER70-S2 and about 8 CFH. Now we're cookin' with gas. Plenty of power for this, but where it was three layers I did find I had floored it for a little bit. I would say most was done around 100 amps. This little machine does as good as any other DC TIG I've used. Smooth!

    Click image for larger version. 

Name:	Toro 2.JPG 
Views:	846 
Size:	71.2 KB 
ID:	9381 Click image for larger version. 

Name:	Toro 3.JPG 
Views:	856 
Size:	79.3 KB 
ID:	9382 Click image for larger version. 

Name:	Toro 4.JPG 
Views:	849 
Size:	95.8 KB 
ID:	9383 Click image for larger version. 

Name:	Toro 5.JPG 
Views:	847 
Size:	102.2 KB 
ID:	9384

    Welded everything up and shot on a little paint while it was still warm enough to get it to dry. It's a bit on the chilly side tonight. And the finished repair, ready to go out and find a new way to break something.

    Click image for larger version. 

Name:	Toro 6.JPG 
Views:	860 
Size:	90.1 KB 
ID:	9385 Click image for larger version. 

Name:	Toro 7.JPG 
Views:	833 
Size:	95.0 KB 
ID:	9386
    Long arc, short arc, heliarc and in-the-dark!

  2. #2
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Nothing like working around smelly chemicals I can tell by the rust good welding job.
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  3. #3
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Kempy View Post
    Nothing like working around smelly chemicals I can tell by the rust good welding job.
    And that's after pressure washing it for at least 15-20 minutes! It was covered with this awful blue dye, stuff gets everywhere.
    Long arc, short arc, heliarc and in-the-dark!

Similar Threads

  1. Project 2 from Youngnstudly. Category: General Welding Repair
    By youngnstudly in forum Welding Repairs
    Replies: 7
    Last Post: 02-01-2013, 05:34 AM
  2. Project#3 from CGCINC. Category: General Welding Repair
    By CGCINC in forum Welding Repairs
    Replies: 5
    Last Post: 12-11-2012, 06:33 PM
  3. Project 2 from Rambozo. Category: General Welding Repair
    By Rambozo in forum Welding Repairs
    Replies: 5
    Last Post: 11-21-2012, 07:48 PM
  4. Project 1 from Rambozo. Category: General Welding repair
    By Rambozo in forum Heavy Equipment and Commercial Projects
    Replies: 14
    Last Post: 08-01-2012, 12:45 AM
  5. Project 1 from CGCINC: Category: General welding repair
    By CGCINC in forum Welding Repairs
    Replies: 15
    Last Post: 07-17-2012, 02:24 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •