  1. #10

    Default

    Ok, I almost finished up the Harbor Freight 20 ton Hydraulic press upgrade to 35 tons. All I have to do now is reinforce the frame on the sides and paint. I should be good up to 75 tons with this now.

    Here is what I did:

    Reinforced the top with 5/16 plate on both sides.

    Reinforced the bed with 5/16 plate on both sides.

    Added spacers to the frame to keep the bed straight.

    Updated to 1 inch grade 8 pins for the bed.

    Added 3/4 inch rod at the bottom to stiffen up the frame.

    Added a SWAG OFF ROAD press brake.....very nice.

    Added an air/hydraulic 32 ton jack which actually has a rating of 70,400 lbs. (35.2 tons actual)

    Here are the photos:

    Click image for larger version. 

Name:	full.jpg 
Views:	951 
Size:	70.5 KB 
ID:	9450Click image for larger version. 

Name:	bed.jpg 
Views:	1020 
Size:	38.7 KB 
ID:	9451Click image for larger version. 

Name:	brake.jpg 
Views:	1061 
Size:	98.5 KB 
ID:	9452Click image for larger version. 

Name:	BRAKE2.jpg 
Views:	851 
Size:	96.1 KB 
ID:	9453

    The SWAG press brake is a great little kit. Very easy to put together and works great.

    If you can find the Harbor Freight hydraulic press on sale, then it is worth updating to a heavier duty version. Plus if you can find a good air / hydraulic bottle jack at a good price, then this is the way to go. But if you can't, then building your own is probably a better rout. Overall, this press now rocks.
    Last edited by Steve; 02-14-2013 at 02:35 AM.
    Powertig 250EX
    Powerplasma 50
    Hobart Handler 210 with spoolgun
    Cobra 2000 / Henrob O/A torch
    Drill press / metal brake / 36 ton air hydraulic press
    Franzinated modified Craftsman 33 compressor
    Lots of other metal working tools

Similar Threads

  1. Removing the Ram Slop from a Harbor Freight 20 Ton Press
    By fyidiy in forum Other Custom Fabrications
    Replies: 18
    Last Post: 08-11-2017, 02:50 PM
  2. Harbor freight Mig wire...stay away!
    By Steve in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 23
    Last Post: 02-14-2013, 04:35 AM
  3. Upgrading a Harbor Freight 20 Ton Press
    By Scooter in forum Other Custom Fabrications
    Replies: 10
    Last Post: 06-11-2011, 03:14 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •