I recently purchased a I-MIG200. Haven't had a chance to play with it until today. First I had to pick up a bottle of 75/25 and wire from Praxair. Then I bought a plug, and off I went. My biggest hurdle was finding out what worked for me with the settings. Once I got that nailed down, off to welding I went.
I am not using the stock gun. I haven't even took it out the box. I bought a Tweco gun because it was longer. I really like it.
Overall, I have to say that this machine is a really good buy. I've used it about a hour straight, and no issues at all. It's a handy little machine! I'm am pumped now that I have her running and it's working flawlessly. If you are looking for a MIG welder, I say this is the way to go.
Here are a few pics.
The machine!
Tweco gun
Welds....
![]()











Reply With Quote