    Default Review of my new I-MIG 200.

    I recently purchased a I-MIG200. Haven't had a chance to play with it until today. First I had to pick up a bottle of 75/25 and wire from Praxair. Then I bought a plug, and off I went. My biggest hurdle was finding out what worked for me with the settings. Once I got that nailed down, off to welding I went.

    I am not using the stock gun. I haven't even took it out the box. I bought a Tweco gun because it was longer. I really like it.

    Overall, I have to say that this machine is a really good buy. I've used it about a hour straight, and no issues at all. It's a handy little machine! I'm am pumped now that I have her running and it's working flawlessly. If you are looking for a MIG welder, I say this is the way to go.

    Here are a few pics.

    The machine!


    Tweco gun


    Welds....





    Purple Fabricator 211i

  2. #2
    Join Date
    Jan 2013
    Location
    Minneapolis, MN
    Posts
    80

    Default

    Did you clean the railing post first? Just curious why the splatter? I'm guessing you were either bunring the paint off or it was windy out blowing the shieling gas. Seems like a nice unit! Thanks

  3. #3

    Default

    The wind was blowing pretty good. I think I need to bump up the psi.
    Purple Fabricator 211i

  4. #4

    Default

    When I was first learning with my IMIG I didn't take the time to prep the metal and it worked ok. But once I spent some time grinding down to bare metal it was like a new machine. Do yourself a favor and clean that metal and give it a go to see what you think.
    IMig 200

  5. #5
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    I've been looking at Everlast IMIG units for awhile now, and I'm jealous of your new IMIG 200! I think I really want to step up to something over 200 amps though, and right now the only thing stopping me from doing that is $1700 and enough free space to store the welder! Just a few "minor" details that need to be ironed out...using a steam roller, or 5!
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  6. #6

    Default

    Have you tried using it on 115v yet? I'm curious how it will perform on 115v.
    Everlast PowerTIG 225LX
    Everlast Power IMIG 200

  7. #7

    Default

    Yea. I plan on using it in the field so I may run across a situation where I dont have 220v. Several locations ive needed to weld only had 460v 3phase and 120v. So I was curious if there were any performance differences between 120v and 220v other than duty cycle and max amps. I had a hobart handler 120 mig welder and it welded like #### no matter how I set it I tried everything!

    Sent from my SGH-T889 using Tapatalk 2
    Everlast PowerTIG 225LX
    Everlast Power IMIG 200

Similar Threads

  1. Powerarc 140 review
    By atatro in forum Stick Welding (SMAW)
    Replies: 40
    Last Post: 06-13-2012, 02:12 PM
  2. 256 Initial review
    By Tony_F in forum Customer Testimonials
    Replies: 14
    Last Post: 03-11-2011, 10:45 PM
  3. 3 month review
    By mdkrusemark in forum Customer Testimonials
    Replies: 7
    Last Post: 02-12-2011, 09:54 PM
  4. PowerPlasma 70 review
    By GWD in forum Everlast Plasma Cutters (PAC)
    Replies: 7
    Last Post: 12-04-2010, 01:10 AM
  5. Super Cut 50 Review
    By WAYNESWORLD in forum Everlast Plasma Cutters (PAC)
    Replies: 17
    Last Post: 12-28-2009, 04:54 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •