    I've got a cheap 4x6 Clarke bandsaw and I'm needing a new blade. What blades do you all recommend for speed of cut? Longevity is second to cut speed. I love being able to set up the saw and turn it on and go work on something else but my current blade is so slow that I've just been using the plasma cutter which ends up with about as much time grinding a smooth edge. I'm still not very good making straight cuts with the plasma.
    IMig 200

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Sandvik or other quality Bi-Metal blades are worth the extra they cost, both in cut speed and blade life.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    I use Supercut blades in my metal band saws 14 or 18 TPI and wood band saws they have performed well with no problems. Bi metal vari tooth blades are great also but for heavier applications and most need coolant.

    Supercut is in Idaho blades are made in USA , I have seen there blades at the local HF
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  4. #4

    Default

    I'll see if I can find the guys card. I bought one some time ago, couldn't find the emails or info on it.

    But this one has been used a lot, and still cuts great. They sold me one at a discount to try it. Have not killed it to get more. It has some type metal M## (I think two numbers), but i googled it back then and heard all good and very impressed with the blade.

    Will post it if I find it. Like said, a quality blade is worth it when cutting metals.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  5. #5

    Default

    I bought some cheap blades to try and save a few bucks..... Junk! Didn't last very long so you get what you pay for!
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  6. Default

    I bought a bunch of Lennox bi-metal blades and really like em. The port-a-band I have didn't use to cut anything and now it goes through pipe and tubing like butter. I converted a Craftsman 14" wood bandsaw to cut metal, and only had one issue with the blade after the conversion. It was taking forever to go through a piece of 1/4 plate and I was starting to have a bad feeling about the blade. Turns out I installed the blade with the teeth facing the wrong way. Still made it about 4 inches into the piece with the teeth pointing up instead of down. After I flipped it around, took about 20 seconds to finish the other 4 inches and has worked great since.
    Poewr I-Mig 205P
    Powertig 185

  7. #7

    Default

    Quote Originally Posted by agent4573 View Post
    I bought a bunch of Lennox bi-metal blades and really like em. The port-a-band I have didn't use to cut anything and now it goes through pipe and tubing like butter. I converted a Craftsman 14" wood bandsaw to cut metal, and only had one issue with the blade after the conversion. It was taking forever to go through a piece of 1/4 plate and I was starting to have a bad feeling about the blade. Turns out I installed the blade with the teeth facing the wrong way. Still made it about 4 inches into the piece with the teeth pointing up instead of down. After I flipped it around, took about 20 seconds to finish the other 4 inches and has worked great since.
    Blade on backwards,,,lol,,,I hold the record for the longest time to cut a piece of 11/2 inch aluminum round bar,,,1 hour 40 minutes,,,before I realized it was on backwards,,,to top that off my neighbour borrowed my chainsaw and returned it with the blade on backwards,,,it ran like that until I figured it out,,,these things can happen,,,duh,,,the obvious sometimes eludes us
    Some of those lies people tell about me, are true

  8. #8
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    Quote Originally Posted by geezer View Post
    Blade on backwards,,,lol,,,I hold the record for the longest time to cut a piece of 11/2 inch aluminum round bar,,,1 hour 40 minutes,,,before I realized it was on backwards,,,to top that off my neighbour borrowed my chainsaw and returned it with the blade on backwards,,,it ran like that until I figured it out,,,these things can happen,,,duh,,,the obvious sometimes eludes us
    Now that's funny! It's not so bad when you catch these silly mistakes immediately, or if you're tired, mad, stressed, (insert other reason for being absent minded), but I hate overlooking the most obvious problem for a long period and wasting time for no reason! It's even worse when you look like a dummy in front of others, or a clueless female sees the problem, points it out, and then brings it up every chance she gets (just to drive you crazy!)!

    I'm interested in fitting a 3/4" wide blade to my portable bandsaw and someone I know said they found those blades online (pre-made), but I have yet to find them in 3/4" width. I might just make some out of blade stock like we used to do at work. The saw will have to be slightly modified so that the blade won't flex and break, but I think it might work out okay. I'll have to experiment a little and see.
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  9. #9
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    I use Lennox neo-type, (in 1/2" x .025") which is stocked by my local "sharp shop", and sold at a reasonable price by the foot, in a variety of teeth pitches. I have tried 24 teeth per inch, and 18 teeth per inch, and prefer the 18 (which works even on very thin steel downspout sheetmetal.) This works on my older craftsman industrial bandsaw (something like a 3"x6" capacity, which takes a 5 foot long blade) when I get it set up properly with enough blade tension. I've done some good and bad blade welds myself with TIG welding, but it's tricky. Getting a good, smooth blade weld that doesn't "catch" as it goes through the cut is important. I'm trying out having the local sharp shop use their blade welding machine for me on the next one.
    Last edited by jakeru; 02-03-2013 at 03:14 AM.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  10. #10
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    I'm going to try getting a few old broken blades from my past employer since the current shop foreman doesn't repair the broken blades (we used to keep like 15 of them around for those "rainy day" repair projects, but it never rained). The blade stretch out is over 100" for that bandsaw and we never kept the broken blades that were missing a ton of teeth or were totally useless.

    In a shop where 20+ employees from other departments had access to the shop tools, there were more than a few idiots (mis)using the equipment by trying to cut sharp curves or using force to cut things. You could tell they were idiots because we posted a brightly colored 20"x20" sign right on the front of the saw that read:"Don't force the material through, LET THE BLADE DO THE CUTTING!!!"
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  11. #11

    Default

    I like Lenox and DoAll blades. When you temper the blade properly they seem to last a long time.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

Similar Threads

  1. Recommend a Torch?
    By Buggy Chief in forum TIG Welding (GTAW/GTAW-P)
    Replies: 18
    Last Post: 02-04-2012, 08:55 PM
  2. Cutting grader blades
    By bobwills in forum General Welding Questions
    Replies: 3
    Last Post: 12-11-2011, 06:49 PM
  3. Looking to get smaller torch soon, what do you recommend?
    By Mark in forum TIG Welding (GTAW/GTAW-P)
    Replies: 12
    Last Post: 11-25-2011, 08:34 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •