  1. Default quick disconnect male fitting

    hello what size is the argon male quick disconnect fitting for the tig torches? Do any online venders sell it?

    Anyone use a regular airline quick disconnect for swapping torches instead?

    thanks

  2. #2

    Default

    Everlast sells them, just call and tell them what you need.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. Default

    Hi thanks is it only available from Everlast? I am in canada and i'd like to buy the fitting locally. Seems a little silly to have a fitting on the machine that can only be bought from everlast.

    Why not add it to the online store?

  4. #4
    Join Date
    Jan 2013
    Location
    Minneapolis, MN
    Posts
    80

    Default

    Maryland Metrics(Male quick connect fitting)
    Rectus 21KA Hose Barb (brass) p/n 21SFTF05MXX 1x$1.25

    http://mdmetric.com/rectus/products/...ka/default.htm

  5. #5

    Default

    Arc-Zone gave me these part numbers to the fitting for everlast machines

    CK-1006
    Fail Safe Ferrule.
    Note: For use with CK-2564 Quick-Release Male Hose Plug.
    CK-2564
    Quick-Release Male Hose Plug. Note for use with CK-1006 Fail Safe Ferrule.

    It's about 8.00$ for both 6 for the connector and 2 for the ferrule you could use a small pipe clamp also

  6. #6

    Default

    Hi -

    For the gas connection you'll have to cut the threaded end off your new torch gas line and install a barbed QD. You can get these barbed QD's from weldingdirect.com, Part number 501N0114. I couldn't find a right hand female threaded connector with the correct QD on the other end. Arczone has one that looks right for the gas line but it IS NOT. QD is too small (P/N ZHCK-G won't work).

    Hope this helps

Similar Threads

  1. POWER PRO 205 Quick disconnect to switch from compressed air to argon
    By cjschwartz in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 20
    Last Post: 02-02-2024, 08:31 PM
  2. Quick connect gas fitting?
    By Dsl power in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 02-18-2014, 09:52 PM
  3. Everlast Tig Torch Quick disconnect fittings 9mm
    By 70Mav in forum Buy, Sale or Trade
    Replies: 10
    Last Post: 03-21-2013, 07:46 PM
  4. Hose barb to quick disconnect fitting
    By AWDnot2 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 12-21-2012, 08:40 AM
  5. Quick connect gas fitting
    By Steve in forum TIG Welding (GTAW/GTAW-P)
    Replies: 11
    Last Post: 11-09-2011, 05:49 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •