    I bought an old 1950's lathe about a year ago and it was damaged pretty bad during shipping. The lag bolts that secured it to the bottom of the crate had broken off, allowing the lathe to "float" inside the crate during shipping. The lid on the headstock was busted in half along with all the (expensive) crank handles, the hand wheel, and the half nut lever. I took care of everything myself besides the cast iron lid.

    When my TIG foot pedal started acting up the other day, I knew I was out of (unusable junk) scrap to run test beads on and figured "Why not weld the lid for my lathe?" So I did. The cast iron stick electrode's were used due to that being all that Airgas had in stock.

    I started by stripping the paint off, mocking the part up on the lathe, and marking each half with a Sharpe for position. Next I ground a vee along both halves of the break, ground areas down that I thought would introduce impurities, removed a few cracks and a large chunk of cast iron that was ready to break off, and preheated everything. Two small tacks were placed on the backside to hold the assembly so I could flip it over and weld the front side. A drop of water was used to test the temperature of the cast iron before (and during) welding since I have no temp gun or temp sticks/crayons sitting around. If the water vaporized instantly, I let the cover cool until it would produce a light "sizzle." Certainly not accurate, but the propane torch flame (that was used to preheat) turned the part gold before it was it was too hot to touch, so I couldn't go off color alone.

    I welded in a root pass using approx. 1" stitches and skipping around, letting the lid cool a few minutes between welds. The last 1/2" (going down the sides) had a large gap due to the hairline cracks I ground out before welding, so I saved those areas for last. The second pass was welded in 3/4" stitches and I tried to use the coldest weld puddle I could while building up the weld with filler. The part got hot a lot quicker than I expected, so I ended up taking numerous breaks between welds. I had to grind out one area of the root pass (where I removed that chunk of cast iron) due to small impurity that formed, but the other side welded really clean.

    Upon flipping the part over, I noticed that my root pass didn't penetrate much towards the underside of the cover (which was almost 3/8" thick), so against my better judgement I welded a quick pass in to fill the bottom side cavity. I never like doing that after welding from the front side, but I just couldn't leave it like that.

    Aside from a few minor low spots left by my 2nd pass (which I filled in easily), the rest of the cover sanded down smoothly. Past experience has told me that welding cast iron is never predictable, but at least this piece doesn't see the extreme temps of cast iron engine parts, or the pressures and flexing that vises and fixtures see. I will epoxy a small 10 ga plate on the underside to cover the weld and possibly keep it more rigid, and add some foam gasket around the opening to prevent the lid from slamming shut and breaking again. I ran out of sanding drums for the Dremel tool, so the backside needs to be smoothed out more.

    I need to prime this and see if I shaped it as good as I think I did (LOL). Cost for the electrodes was $8.99 and it took just under an hour from start to finish, including quite a few cool down periods.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	IMG_1058.jpg 
Views:	751 
Size:	138.0 KB 
ID:	9292   Click image for larger version. 

Name:	IMG_1059.jpg 
Views:	644 
Size:	141.2 KB 
ID:	9293   Click image for larger version. 

Name:	IMG_1060.jpg 
Views:	710 
Size:	150.5 KB 
ID:	9294   Click image for larger version. 

Name:	IMG_1062.jpg 
Views:	701 
Size:	136.7 KB 
ID:	9295   Click image for larger version. 

Name:	IMG_1080.jpg 
Views:	669 
Size:	142.6 KB 
ID:	9296  

    Click image for larger version. 

Name:	IMG_1077.jpg 
Views:	699 
Size:	144.9 KB 
ID:	9297   Click image for larger version. 

Name:	IMG_1081.jpg 
Views:	674 
Size:	138.2 KB 
ID:	9298  
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  2. #2

    Default

    Turned out great... nice work.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #3
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    Thank you zoama. I hope it works without cracks or breakage occurring in the future! I guess I can always buy a used cover later on when I have an extra $25-$50, if it does indeed fail. Fingers are crossed anytime I weld cast iron.
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  4. #4

    Default

    I did not read the whole post. But if it's a cover? More than one pass I think I saw, and bottom the side has good penetration. It will last a long time.

    The cleanup work to me was nice, but I get yelled at for grinding welds here. I like it to look like all one part, other her like you to see the welds. My vote, looks great (like one part).
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  5. #5
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Looks great. Is that an Atlas? Looks a little familiar.
    Long arc, short arc, heliarc and in-the-dark!

  6. #6
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    Quote Originally Posted by Rambozo View Post
    Looks great. Is that an Atlas? Looks a little familiar.
    It certainly is! It's a little 6-18 that I bought fairly reasonably and rebuilt. This piece is the last part I need to complete this lathe, so I'm happy.
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  7. #7

    Default

    Man, I love stuff like this. This embodies why I want to weld: one more skill that lets me A) create exactly what I want, customized to my needs or B) repair something that's broken, allowing me to keep using something that's 99% totally fine without throwing it away and getting a new one. I love it.

    Very nice work! I agree with everlastsupport - I also like the idea of hiding the welds in cases like this, making it look like it was never broken. Invisible repair. On certain things (mostly new fab), I like the idea of showcasing the welds. For me, it depends on the situation and the piece.
    Everlast PowerArc 140ST

  8. #8

    Default

    Oh yeah. That's what we're talking about. Great job on the repair!

Similar Threads

  1. Project 3 from Rambozo. Category: General Welding Repair
    By Rambozo in forum Welding Repairs
    Replies: 2
    Last Post: 02-10-2013, 01:11 PM
  2. Project#3 from CGCINC. Category: General Welding Repair
    By CGCINC in forum Welding Repairs
    Replies: 5
    Last Post: 12-11-2012, 06:33 PM
  3. Project 2 from Rambozo. Category: General Welding Repair
    By Rambozo in forum Welding Repairs
    Replies: 5
    Last Post: 11-21-2012, 07:48 PM
  4. Project 1 from Rambozo. Category: General Welding repair
    By Rambozo in forum Heavy Equipment and Commercial Projects
    Replies: 14
    Last Post: 08-01-2012, 12:45 AM
  5. Project 1 from CGCINC: Category: General welding repair
    By CGCINC in forum Welding Repairs
    Replies: 15
    Last Post: 07-17-2012, 02:24 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •