  1. Default welding ?

    i have a question about welding some 1/4 inch plate to 3/8 inch thick wall pipe would i be better to use stick or tig ?
    i will have a PowerUltra 205
    this will be on a smoker so it dont have to be strong just look nice and hold air/smoke

  2. #2

    Default

    Tig will give you a pretty weld,,, but 7014 rod looks good too,,,It's a smoker not rolex,,,so how nice do it have to look,,throw some heat resistent paint on it and who will be looking at the welds
    Some of those lies people tell about me, are true

  3. #3
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Quote Originally Posted by travis View Post
    i have a question about welding some 1/4 inch plate to 3/8 inch thick wall pipe would i be better to use stick or tig ?
    i will have a PowerUltra 205
    this will be on a smoker so it dont have to be strong just look nice and hold air/smoke
    Clean the plate and pipe and Tig it, it will look better and Tig penetrates very well 1/4 to 3/8 full power ahead.
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

Similar Threads

  1. First Welding Project - You guessed it... a welding cart
    By EmptyNester in forum Hobyist Projects
    Replies: 19
    Last Post: 10-12-2011, 03:30 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •