Share
Results 1 to 18 of 18

Thread: mig 250p

  1. Default mig 250p

    Hello I am thiking of buying a 250p and was wondering if anyone had one and what they thought of it. Also any pics of the welds

  2. #2

    Default

    I have one that I use often but I'm a novice welder with no formal training. I like it especially after changing the oem torch to a 20' profax.
    I don't have any weld pics right now but I may put some up in the next couple of weeks. Actual voltage range is 14.5 to 28.5
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #3

    Default

    The 205P and 250P are both close units if you are looking at them.

    I have a 200, 205P and 250P (we use them almost everyday, even weekends). The 250P, I like, as I can roll it where I need it (I have a benzil 15AK on it, but the torch that comes with it is fine; I like smaller size).. No cart required on the 250P. 205P you will need to make a cart (or buy one) .

    The 205P welds as nice, just a little less power.

    Pictures of welds? That will only show you how I weld not you. Looks for user Chadrock, almost all his projects are 200, 205P and 250P and all the welds looked the same.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  4. #4

    Default

    I just welded with mine for the first time yesterday.
    I really like it.
    At my work, I weld 8 hours a day, so I know how to weld.
    I haven't dabbled with the pulse yet, or the stick welding yet.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	01-26-13 Welder 10.jpg 
Views:	640 
Size:	148.2 KB 
ID:	9253  
    Power I-MIG-250P

  5. #5

    Smile

    Another picture.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	01-26-13 Welder 16.jpg 
Views:	619 
Size:	140.5 KB 
ID:	9254  
    Power I-MIG-250P

  6. Default

    Looks good Mark thanks. I have 3 stick machines so dont really need the stick part.

  7. #7

    Default

    At work, I use .045 wire, with a 90/10 mix of gas.
    I run 30 amps/29ish volts=3 pass, 12 millimeter welds.
    So, coming home and using my little 250p is a bit different
    Power I-MIG-250P

  8. #8

    Smile

    I'm making a cart for my 250P.
    I know, it has wheels, but I can't leave good enough alone.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	01-26-13 Welder 15.jpg 
Views:	538 
Size:	141.7 KB 
ID:	9255   Click image for larger version. 

Name:	01-26-13 Welder 13.jpg 
Views:	547 
Size:	141.1 KB 
ID:	9256  
    Power I-MIG-250P

  9. #9

    Default

    I went out to the shop and made a little demo weld. 11 gauge HR steel, 19v, 220 wire speed on the display (reads amps when welding) 75/25 gas.
    I haven't learned how to minimize the BBs Click image for larger version. 

Name:	IMG_1312.jpg 
Views:	739 
Size:	145.3 KB 
ID:	9258 Any tips would be appreciated.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  10. Default

    run it on pulse that should get rid of them

  11. #11

    Default

    Quote Originally Posted by steel View Post
    run it on pulse that should get rid of them
    I haven't learned to use the pulse feature, is that commonly used in short circuit ? You can click on the thumbnail pics for a larger view, it's a fairly high res pic.
    Last edited by zoama; 01-27-2013 at 10:40 PM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  12. #12

    Default

    Quote Originally Posted by zoama585 View Post
    I went out to the shop and made a little demo weld. 11 gauge HR steel, 19v, 220 wire speed on the display (reads amps when welding) 75/25 gas.
    I haven't learned how to minimize the BBs Click image for larger version. 

Name:	IMG_1312.jpg 
Views:	739 
Size:	145.3 KB 
ID:	9258 Any tips would be appreciated.
    Excess Gun angle increases BB.s Pushing may help as well. You can tune the arc force, and reduce the wire speed or increase the voltage to reduce the BB's. After optimizing these settings, you can also go to an 80/20 or in my case a C18(Air Gas proprietary blend). Try dropping your wire speed to 200...What brand wire and wire size are you using?

  13. #13

    Default

    Quote Originally Posted by performance View Post
    Excess Gun angle increases BB.s Pushing may help as well. You can tune the arc force, and reduce the wire speed or increase the voltage to reduce the BB's. After optimizing these settings, you can also go to an 80/20 or in my case a C18(Air Gas proprietary blend). Try dropping your wire speed to 200...What brand wire and wire size are you using?
    I'm running the silver esab wire you recommended .035. Gun angle was close to 90 deg My lws only offers 75/25 or tri mix, they looked at me like I was an alien when I asked for c18 or 80/20
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  14. #14

    Default

    Ok, you need a lean, not a straight down angle. Start by pushing it slightly. 15 to 20 degrees should do it. The most of the BB's if there are many, will bounce in front of the weld and get reabsorbed. Keep your standoff as close as practical, 1/2" or so. Too long of a stand off can create spatter. But again, dialing the wire speed down will help. Most people tend to run too much because they feel they will get a hotter weld. But it's like trying going to a hot dog eating contest...eventually something is going to spew all over the place at too fast of a feeding rate. And dialing the arc force control will likely give you the most change in spatter. I run mine about 3 oclock on the small imig. Not sure if that will translate well or not. Mike may have more input.

  15. #15

    Default

    I went out and did a few more tests, settings are all over the place but I thought it would help to narrow down my problems. Torch angle is still almost straight up and down because I hadn't read the last advise yet.
    From left to right, Pic 1 is 19.5v 220 wire speed 5 arc force__ Pic 2 is 19v 200 wire speed 5 arc force__ Pic 3 is 19v 200 wire speed 3 arc force__ Pic 4 19v 210 wire speed 7 arc force.
    Click image for larger version. 

Name:	IMG_1315.jpg 
Views:	738 
Size:	146.3 KB 
ID:	9260Click image for larger version. 

Name:	IMG_1316.jpg 
Views:	703 
Size:	146.5 KB 
ID:	9261Click image for larger version. 

Name:	IMG_1317.jpg 
Views:	654 
Size:	146.8 KB 
ID:	9262Click image for larger version. 

Name:	IMG_1318.jpg 
Views:	693 
Size:	146.7 KB 
ID:	9263

    Also, what causes the rust color around the weld ? The pieces were all cleaned with a coarse 8" wire wheel on a grinder before welding. 75/25 at 12 lpm. I usually run it at 10 lpm but increased it on these welds and it didn't make much difference.
    All pieces were the same size and temperature. Pics are high res... for those who don't know how to zoom in, click on the thumbnail then click on the pic that opens, hold the Ctrl key on your keyboard while you roll the mouse wheel forward.
    Last edited by zoama; 01-28-2013 at 12:14 AM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  16. #16

    Default

    Last one looks best. I'd go up to 7.5 and lower wire speed to 190. Leave voltage where it is. The reason you are getting the smoked appearance is partly because of the CO2 and the other two parts....One is because of your gun angle is forcing it uphill( notice the spatter on the up hill side?) You may be holding 90 in one plane but angling it on the other so that the arc is pushing up rather than forward. The other is because you haven't ground the metal to lay a clean pass. Wire wheels don't cut it...all you are doing is polishing mill scale...sort of like polishing pooh.
    Last edited by performance; 01-28-2013 at 12:43 AM.

  17. #17

    Default

    Quote Originally Posted by performance View Post
    Last one looks best. I'd go up to 7.5 and lower wire speed to 190. Leave voltage where it is. The reason you are getting the smoked appearance is partly because of the CO2 and the other two parts....One is because of your gun angle is forcing it uphill( notice the spatter on the up hill side?) You may be holding 90 in one plane but angling it on the other so that the arc is pushing up rather than forward. The other is because you haven't ground the metal to lay a clean pass. Wire wheels don't cut it...all you are doing is polishing mill scale...sort of like polishing pooh.
    All pieces had the ground clamp on the top left corner causing them to tilt back a little. I'll work on it some more tommorow, thanks for the help.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  18. #18

    Default

    sort of like polishing pooh
    Haven't we all done that a time or two LOL
    Power I-MIG-250P

Similar Threads

  1. 250p Spray Arc
    By zoama in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 11
    Last Post: 08-14-2024, 02:09 AM
  2. Tig 250p problem
    By jakesporting in forum TIG Welding (GTAW/GTAW-P)
    Replies: 14
    Last Post: 09-22-2016, 11:51 AM
  3. Power I-MIG 250p
    By Yofish in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 0
    Last Post: 02-25-2015, 04:25 AM
  4. i-Mig 250, or i Mig 250p, or i-Mig 400?
    By John71a in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 3
    Last Post: 02-21-2014, 12:16 AM
  5. 250p ???
    By txshockwave in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 7
    Last Post: 01-05-2013, 01:48 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments