Share
Results 1 to 4 of 4

Thread: Filler rod sticks to work

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default Filler rod sticks to work

    When I tried welding chromoly tubing my ER70S-2 sticks to the work everytime I dab it into puddle. What I'm I doing wrong?

  2. #2

    Default

    Quote Originally Posted by gree box View Post
    When I tried welding chromoly tubing my ER70S-2 sticks to the work everytime I dab it into puddle. What I'm I doing wrong?
    What size filler and what size tube ?
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. Default

    I'm using 3/32 and welding 1 5/8 .090 wall pipe. Is the rod grounding to the metal?

  4. #4

    Default

    when a filler rod sticks to the weld you don't have enough heat in the puddle to melt the filler rod off,,,welding a thin wall pipe will not give you a big enough puddle to melt the filler rod unless the filler rod is very thin,,,try using a thinner filler rod that will melt off and flow into the puddle without cooling the puddle and sticking..
    Some of those lies people tell about me, are true

Similar Threads

  1. New to welding. Which filler rod?
    By Xman4u in forum General Welding Questions
    Replies: 2
    Last Post: 01-16-2015, 12:43 PM
  2. USING FILLER ROD Poll
    By Titan winch in forum General Welder Questions
    Replies: 16
    Last Post: 08-30-2011, 12:08 PM
  3. TIG Filler
    By bigjoeinkg in forum TIG Welding (GTAW/GTAW-P)
    Replies: 13
    Last Post: 07-18-2011, 10:50 PM
  4. filler rod stubs
    By dgarnier in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 04-28-2011, 10:02 PM
  5. Which filler Rod for what application?
    By jameswswanson in forum General Welder Questions
    Replies: 2
    Last Post: 04-28-2011, 12:54 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •