Share
Results 1 to 5 of 5

Thread: Magnets and IMig don't Mix

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default Magnets and IMig don't Mix

    I've been working on a big project with my IMig 200 and the welder started acting real funny after a few hours. I took everything apart checked the drive tensions and the gas output to no avail. I gave up for the night and started cleaning up the space and realized that my dad stuck one of my heavy duty magnetic clamps to the back of the piece that I was working on. I popped it off and gave it another shot and everything worked as it should! Sometimes it's the simplest things that cause you to lose the most time. I now know the sound and will be an easy fix in the future. Other than that I just made it through 2 lbs of wire in about three days of working and started my first 10 lb roll. I'm really liking the IMig!
    IMig 200

  2. #2

    Default

    Also do not forget heat will kill your magnets too.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  3. #3
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Well I glade you like the welder I am looking at buying one soon, it's back to what I said yesterday it is usually not the welder but I forgot about magnets they do cause a lot of problems in welding mainly in Tig holding steel parts together and welding near them. Good luck on the projects.
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  4. #4
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    So the presence of a big enough magnet caused arc blow? I'd heard of this in SMAW, never thought about it for GMAW.

    And did your Dad do it on purpose as a prank? ;-)
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  5. #5

    Default

    Quote Originally Posted by DaveO View Post
    So the presence of a big enough magnet caused arc blow? I'd heard of this in SMAW, never thought about it for GMAW.

    And did your Dad do it on purpose as a prank? ;-)
    It *really* messes with TiG welding. Screws up the arc and the puddle flow.
    -------------------------------------------
    Spike Customs, Inc.
    Fresno, CA 93727
    ph- 559-549-RIDE(7433)
    -------------------------------------------
    -Follow me on twitter!-

Similar Threads

  1. Imig 205//210
    By Doc Pete in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 2
    Last Post: 01-19-2017, 12:25 PM
  2. Tig welding with magnets around and aluminum cleaner
    By Steve in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 08-05-2013, 07:21 PM
  3. IMig 200 For Sale
    By SeanMurphy265 in forum Buy, Sale or Trade
    Replies: 2
    Last Post: 04-03-2013, 01:02 AM
  4. Welding magnets vs clamps
    By Trip59 in forum General Welding Questions
    Replies: 18
    Last Post: 10-11-2011, 05:07 AM
  5. power IMIG 205
    By Wrenchtamer in forum Customer Testimonials
    Replies: 3
    Last Post: 03-04-2011, 01:47 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •