Share
Results 1 to 7 of 7

Thread: Stoodite 21 Tig Rod For Repairing Anvil Top Plate ??

  1. #1

    Default Stoodite 21 Tig Rod For Repairing Anvil Top Plate ??

    I have an older Swedish Kohlswa anvil , it has some chips on the edges of the top plate wondering if this rod would work for repair.

    Stoodite 21 1/8" dia

    I have used it on tooling dies ect.
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by cbmkr View Post
    I have an older Swedish Kohlswa anvil , it has some chips on the edges of the top plate wondering if this rod would work for repair.

    Stoodite 21 1/8" dia

    I have used it on tooling dies ect.
    I'm sure that rod would work fine, but I would have more concerns about the base metal. Any idea of the alloy, carbon content, or hardness? It might require a ton of pre-heat and post welding heat stress relieving to keep from hardening the base metal at the edge of the HAZ. Otherwise you might just create new larger chips to repair.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    Not really sure of the base material for the plate, I know they set them in the mold before they were cast in Sweden. Some of the guys on the anvil forums have welded them up with stick and reground. One of the Everlast forum members i believe blacksmith ?? might have more info.
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  4. #4

    Default

    If its a good anvil, the hammering face should be a heat treated spring steel. The rest of the anvil should be a good quality steel, and the whole top half of the anvil is heat treated. If you do any welding on it, you will need to have it heat treated again, otherwise it will be soft and won't spring back from the hammer blows.
    -------------------------------------------
    Spike Customs, Inc.
    Fresno, CA 93727
    ph- 559-549-RIDE(7433)
    -------------------------------------------
    -Follow me on twitter!-

  5. #5
    Join Date
    Oct 2011
    Location
    Litchfield Park, AZ
    Posts
    370

    Default

    Quote Originally Posted by cbmkr View Post
    I have an older Swedish Kohlswa anvil , it has some chips on the edges of the top plate wondering if this rod would work for repair.

    Stoodite 21 1/8" dia

    I have used it on tooling dies ect.
    Attached is a good link.

    http://www.blksmth.com/Dick's_Shop_Tips.htm

    As for the welding, I think you are talking about Stellite 21 , not Stoodite. I you are just fixing some chips there will not be too much of an issue in localized areas if you have ductal material. If the anvil is martensitic steel and not preheated, you may have some issues.
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

  6. #6

    Default

    Quote Originally Posted by DVA View Post
    Attached is a good link.

    http://www.blksmth.com/Dick's_Shop_Tips.htm

    As for the welding, I think you are talking about Stellite 21 , not Stoodite. I you are just fixing some chips there will not be too much of an issue in localized areas if you have ductal material. If the anvil is martensitic steel and not preheated, you may have some issues.
    No its Stoodite 21, Used it years back for repairing punch and die sets, was just curious if anyone had used it on an anvil. i will just use the same method as i have for years cleaning and pre heating to approx 400-500 deg F before welding. Used to do a brinell hardness test years ago to get a reading , then soften the material to do the repair and harden to the previous spec.
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  7. #7
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by DVA View Post
    As for the welding, I think you are talking about Stellite 21 , not Stoodite. I you are just fixing some chips there will not be too much of an issue in localized areas if you have ductal material. If the anvil is martensitic steel and not preheated, you may have some issues.
    Stoodite is just the Stoody brand name version because Stellite is a trademarked brand as well.
    Long arc, short arc, heliarc and in-the-dark!

Similar Threads

  1. Anvil's That are In Use In My Shop
    By cbmkr in forum Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
    Replies: 6
    Last Post: 08-09-2013, 07:48 PM
  2. Desk Name plate
    By acourtjester in forum Metal Art
    Replies: 1
    Last Post: 01-25-2013, 06:39 PM
  3. Repairing a small cast iron gib key
    By build in forum General Welder Questions
    Replies: 8
    Last Post: 12-13-2012, 02:23 AM
  4. Replies: 2
    Last Post: 08-27-2012, 03:21 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •