  1. Default 256 cutting in and out mid bead

    Welding aluminum...been working fine. Then all the sudden the arc would stop and start. Any ideas?

  2. Default

    Well...it looks like it is a problem with the pedal...if I let off the pedal to about 90% it works fine, 100% and the arc gets scattered. These dammn pedals are junk! this is a replacement, as the original quit working after a few months. Now this one is messed up... aggravating!

  3. #3

    Default

    If you order the SSC pedal from Everlast, $149.00, the machine comes alive!
    Everlast PowerPro 256
    Everlast W300 Cooler
    Everlast Cart 250

    Millermatic 211
    Spoolgun 100
    Miller HD Cart

    Victor 315 Torch sitting on a Harper 830-86 cart

Similar Threads

  1. pulse weld bead vs constant bead
    By fullydrooped in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 11
    Last Post: 02-18-2014, 01:20 AM
  2. DIY dryer for plasma cutting and TIG welding. Dross cutting or TIG electrode fur
    By everlastsupport in forum Welding articles from Professionals (knowledge database)
    Replies: 0
    Last Post: 03-15-2012, 12:08 PM
  3. New Bead Roller
    By acourtjester in forum Personal Projects (no welder required)
    Replies: 7
    Last Post: 06-09-2011, 11:36 PM
  4. Another bead roller conversion
    By Ram48 in forum Other Custom Fabrications
    Replies: 13
    Last Post: 04-27-2011, 02:24 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •