Thread: Best Nozzle for Close Angle Merged Exhaust Tubing?

  1. Question Best Nozzle for Close Angle Merged Exhaust Tubing?

    I made it this far merging a smaller (~2 inch) exhaust pipe into a larger 3 inch pipe (stainless steel), but I could not complete the weld because my #12 nozzle was too big! Is there a better nozzle size you experienced welders would recommend so I can finish the top of this merge section?





    And YES, I tried all different angles with the torch and protruding the tungsten out, it just won't fit .

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Try a #6 gas lens or even a regular collet body, with as much stickout as required to get in there. You can use a foil dam on the other side to help hold the argon. In close areas like that, shielding usually isn't much of a problem. Just dam up the sides with foil and remember argon is heavier than air so it will fill up places like that. You might actually have to back down your flow to keep air from being sucked into the stream. Just pre-flow long enough to fill the area. You have to think about weld access when planing things like that. You can also probably reach that area from inside through your flange with a pencil type torch.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    I agree with rambozo. tin foil is a staple of the professional welding shop. Not only does it work great as an air dam, but you can also fold layers of it together to make a heat shield, or as a spatter blocker if you're MiG welding over something important.

    Aside from that, sometimes you can't get the puddle to go where you want on the tubing without burning holes in the thin wall tubing. On exhaust tubing sometimes its necessary to start building up the weld further up the tube, where you can get better control over the puddle and finally join the two sides of your seam together. On the outside it looks like you just have a longer notch joint than you actually do. This is a common practice when making exhaust systems, and having the extra thickness in those very acute angles certainly helps the longevity of the product. (these tight angles that face into the exhaust flow are the hottest parts odd the exhaust system)

    The weld can be done, tho so don't give up! There's enough room to get a grinder in there and clean it out if you need to re weld.
    The 6g restricted (6gr) test for ships and nuclear pipes makes you weld a stainless sch 160 pipe together boxed between 2 other pipes with a 1/2" clearance and you can't feet to the backside and have to TiG weld the backside of the joint with a mirror and your hands reaching around the bundle of pipes.
    -------------------------------------------
    Spike Customs, Inc.
    Fresno, CA 93727
    ph- 559-549-RIDE(7433)
    -------------------------------------------
    -Follow me on twitter!-

  4. #4

    Default

    Not really relavent to your post directly, but check out this header from Sebastian Domingo of Next Level Racing / NLR Systems.
    I have one of these on teh shelf for my bike. I bought everything to make my own and then jsut decided to buy one of his already done.

    http://www.suzukihayabusa.org/forum/...topic=134596.0
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  5. #5

    Default

    Quote Originally Posted by sportbike View Post
    Not really relavent to your post directly, but check out this header from Sebastian Domingo of Next Level Racing / NLR Systems.
    I have one of these on teh shelf for my bike. I bought everything to make my own and then jsut decided to buy one of his already done.

    http://www.suzukihayabusa.org/forum/...topic=134596.0
    Nice work,,however I have to disagree with the method used to assure a flat surface on the header plate,,,welding here and there to straighten the plate is a hit and miss, trial and error method,,,much simpler to use a press and a straight edge,,,to get it close ,,,then a light pass on a milling machine to assure a flat surface...other than that the header work is very good,,,nice looking product

    As far as welding in a tight area with the tig,,,if the cup won't get you there,,you may want to finish the weld with O/A,,,
    Some of those lies people tell about me, are true

  6. Default

    I agree with Rambozo, a gas lens and a huge stickout will probably work. The aluminum foil trick I've never heard of but sounds interesting. Would probably work just fine too.
    Poewr I-Mig 205P
    Powertig 185

  7. #7

    Default

    Quote Originally Posted by Spike View Post
    The weld can be done, tho so don't give up! There's enough room to get a grinder in there and clean it out if you need to re weld.
    The 6g restricted (6gr) test for ships and nuclear pipes makes you weld a stainless sch 160 pipe together boxed between 2 other pipes with a 1/2" clearance and you can't feet to the backside and have to TiG weld the backside of the joint with a mirror and your hands reaching around the bundle of pipes.
    That just sounds like a pain in the ###.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  8. #8
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    When I have to get into very small places I us standard collects and holders with long cups preheat if possible and set gas flow differently for the small ends just test it on a part to see how it work before doing the big job. Use type B solar flux in side the pipe if stainless steel then you don't have to use argon in the pipe. The flux provents burn throught, ozide inclusions and aids controlled penetration also elimiates porosity. GOOD LUCK
    Click image for larger version. 

Name:	101.jpg 
Views:	745 
Size:	156.4 KB 
ID:	9135
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  9. #9

    Default

    Quote Originally Posted by Kempy View Post
    When I have to get into very small places I us standard collects and holders with long cups preheat if possible and set gas flow differently for the small ends just test it on a part to see how it work before doing the big job. Use type B solar flux in side the pipe if stainless steel then you don't have to use argon in the pipe. The flux provents burn throught, ozide inclusions and aids controlled penetration also elimiates porosity. GOOD LUCK
    Click image for larger version. 

Name:	101.jpg 
Views:	745 
Size:	156.4 KB 
ID:	9135
    lol... nozzle envy.
    -------------------------------------------
    Spike Customs, Inc.
    Fresno, CA 93727
    ph- 559-549-RIDE(7433)
    -------------------------------------------
    -Follow me on twitter!-

  10. #10

    Default

    Quote Originally Posted by Kempy View Post
    When I have to get into very small places I us standard collects and holders with long cups preheat if possible and set gas flow differently for the small ends just test it on a part to see how it work before doing the big job. Use type B solar flux in side the pipe if stainless steel then you don't have to use argon in the pipe. The flux provents burn throught, ozide inclusions and aids controlled penetration also elimiates porosity. GOOD LUCK
    Click image for larger version. 

Name:	101.jpg 
Views:	745 
Size:	156.4 KB 
ID:	9135
    Do those require you turn the flow down a lot?
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  11. #11

    Default

    Quote Originally Posted by geezer View Post
    Nice work,,however I have to disagree with the method used to assure a flat surface on the header plate,,,welding here and there to straighten the plate is a hit and miss, trial and error method,,,much simpler to use a press and a straight edge,,,to get it close ,,,then a light pass on a milling machine to assure a flat surface...other than that the header work is very good,,,nice looking product

    As far as welding in a tight area with the tig,,,if the cup won't get you there,,you may want to finish the weld with O/A,,,
    In this case it is not hit and miss. He makes quite a few of these and pretty much has it down pat. I agree for a one off, but he has the procedure pretty well figured out. THese were from a while ago. He now uses a CNC flange, mostly for appearance. He is currently working on a new version starting with electro polished weld Ells. Should look pretty good.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  12. #12
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    I turn it down a little even when using smaller standard cups but if I get into tough spots I turn it up a little. You have to play around each cup and regulators are a little different and beening water cooled or gas cooled. The longer ones I some times turn it up if I am using a lot of power for the size of cup to help cool it. I use a long post flow to help cool the cup after welding.
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  13. #13
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    This guy gets good results on narrow angle stainless merge collector with what looks like something in the area of a #6-#7 gas lens, and maybe a cup width's worth of stickout; I'd say. (see his stickout @ 1:50)
    http://www.youtube.com/watch?feature...c3AQFHI#t=105s

    Running a cup width's worth of stickout is not hard to do with a gas lens. You can run even more stickout than that if necessary, with the right conditions and setup. Note, if you can set up your workpiece so the tungsten is pointing straight down (1G position), the heavy argon will tend to fall down onto the hot weld metal.) You should of course try and do this work indoors in a still (non-windy) environment.

    If you use a larger diameter cup, you'll probably need to stick your tungsten out further, and use more gas to have it work. A #12 cup may need 30 or so cfh to work best, where a #8 needs 15 or more cfh. A #6 can use 12 cfh or so. The area of the cup increases with the square of the diameter (cup size), and IME, the gas flow should increase proportionally to the area of the cup for best results. The wider cup will shield a wider area of hot metal than the narrower cup. Be sure to run enough pre and post flow. Proper torch angle is also very important. (Don't angle it so that you draft air in next to the hot metal)

    Using a sufficiently small diameter tungsten (I'd recommend 1/16" for what you're doing, not 3/32") and having a pointed, clean, contamination free tip may also be necessary to keep the arc coming off the very end of the tungsten (not off to the side).

    Also - make sure your filler rod is sufficiently small diameter to reach where it needs to go, because if it can't reach the puddle, then the puddles are going to need to grow in size until they can get bridged across by the filler rod. You may need to change your "angle of approach" with the filler rod to get it deep into the groove, where it's needed.
    Last edited by jakeru; 01-15-2013 at 05:04 PM.
    '13 Everlast 255EXT
    '07 Everlast Super200P

Similar Threads

  1. pp 205 plasma don't like being close
    By ogre in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 8
    Last Post: 09-19-2014, 01:29 AM
  2. Replacement gas nozzle
    By DaveO in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 14
    Last Post: 10-23-2012, 03:43 PM
  3. cutting at an angle
    By McClary in forum Everlast Plasma Cutters (PAC)
    Replies: 4
    Last Post: 12-29-2011, 12:01 PM
  4. Replies: 0
    Last Post: 04-29-2011, 05:41 AM
  5. tig torch gas nozzle
    By gwk in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 10-03-2009, 08:28 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •