You are correct that they do look cold. It also looks like you make pretty tight movement which is something I did at first also. I would bet more heat and maybe moving a little faster or in a little bigger strides would make it pretty nice.
You are correct that they do look cold. It also looks like you make pretty tight movement which is something I did at first also. I would bet more heat and maybe moving a little faster or in a little bigger strides would make it pretty nice.