    I also use a CK130 (mine has a flex head). It's a great torch. Easy to maneuver.

  2. #22

    Default

    Quote Originally Posted by zank View Post
    Thank you. That's not brushed. That's as-welded. You can see some straw color where I started to outrun my shielding on the left side of the joint. You can also see a little straw color adjacent to the weld all the way around.
    Yea, on the titanium I could see it, even the very very little in the middle. Very nice TIG weld(s).

    Are you one of the owners of ZCC (ZanK name makes me ask).?

    On the gas lens you can save a little gas and get more stickout. Not a bad deal at all.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  3. #23

    Default

    Yeah, that's me. One man shop here.

  4. #24

    Default

    Quote Originally Posted by zank View Post
    Yeah, that's me. One man shop here.
    Nothing wrong with that, looks like the talent is there to handle it. And better, no one to argue with but you.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  5. #25
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    Quote Originally Posted by performance View Post
    Visibility can be blocked by the larger diameter gas lens...
    But the glaringly obvious issue that I see here is the fact you have ignored the warranty! You should have tested your unit as soon as you received it. IF there are any shipping issues/damage, it will likely be up to you. You are supposed to test and FULLY inspect the unit promplty after receiving it. The reason I bring this up is this also affects our ability to determine what happened to the unit, and will send you past the 30 day warranty period. Please read your warranty if you haven't. http://www.everlastgenerators.com/terms.php
    You're absolutely right Mark. It slipped my mind with all of the other things going on right now, and I take full responsibility for my (lack of) action regarding the warranty. Nothing I can do about it now expect hope that it works!
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  6. #26

    Default

    Your warranty will be in force, but the shipping will be on your dime, especially if it is over 30 days.

  7. #27

    Default

    Quote Originally Posted by performance View Post
    Visibility can be blocked by the larger diameter gas lens...
    But the glaringly obvious issue that I see here is the fact you have ignored the warranty! You should have tested your unit as soon as you received it. IF there are any shipping issues/damage, it will likely be up to you. You are supposed to test and FULLY inspect the unit promplty after receiving it. The reason I bring this up is this also affects our ability to determine what happened to the unit, and will send you past the 30 day warranty period. Please read your warranty if you haven't. http://www.everlastgenerators.com/terms.php
    I did read the warranty, which states Everlast will cover shipping up to 30 days after purchase. My unit was out of coverage by the time it was delivered, which was about 7 weeks after purchase.

    So unless I'm misinterpreting the legalese, I don't have much incentive to test the unit before I'm really ready to use it.


    Sent from my PC36100 using Tapatalk 2
    Just a new guy that wants to make stuff.

    PowerPro 256

  8. #28

    Default

    Well, the incentive is IF you have a problem and you ARE ready to use it, you will not be able to and will be further delayed until it is repaired. In cases where a preorder is made and shipping is delayed, it is counted from the time of shipping. Normally shipping and day of sale are the same.

  9. #29
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Yes - there are downsides to a gas lens:
    http://www.everlastgenerators.com/fo...7233#post37233

    Click image for larger version. 

Name:	IMG_2199 (2).jpg 
Views:	375 
Size:	135.3 KB 
ID:	9029
    Last edited by jakeru; 12-30-2012 at 09:15 PM.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  10. #30

    Default

    Quote Originally Posted by jakeru View Post
    Yes - there are downsides to a gas lens:
    http://www.everlastgenerators.com/fo...7233#post37233
    At $1.79 I wouldn't worry about it. http://www.weldingcity.com/tig-consu...llet-body.html
    Last edited by zoama; 12-30-2012 at 09:20 PM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  11. #31

    Default

    I've been using the cheap gas lenses like what's available from welding city for about a yr now (off and on). I don't think I've ever used a standard collet to tig at all. But just today I got in my new CK130Flex and a Gas saver kit with the pyrex cup. I've fallen in love with these pyrex cups.. I CAN SEE THE ENTIRE PUDDLE! I've only layed one bead tonight after installing it, on some scrap aluminum, but I think it's the most consistent welding I've ever done. Seeing the puddle cool and the keyhole open up is key to knowing when to dip the rod again, with the clear cup I can see everything. I also noticed that the flow of argon is alot smoother through the gas saver kit than the standard gas lenses... Does everyone else with the pyrex gas saver kits notice the same thing over a standard gas lense?
    Everlast PowerTIG 225LX
    Everlast Power IMIG 200

  12. #32
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by Trip59 View Post
    do you read the flowmeter from Everlast at the top, middle or bottom of the ball?
    Been wondering that myself. I've just been going with the middle, figuring that would equalize any error from an incorrect guess.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  13. #33

    Default

    Quote Originally Posted by redbeard View Post
    Been wondering that myself. I've just been going with the middle, figuring that would equalize any error from an incorrect guess.
    I use the least amount that gets me a clean weld in testing, so wherever I read it from first is where I read it every time after, but I think I read it in the middle as well... hadn't thought about it until now.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  14. #34
    Join Date
    Nov 2012
    Location
    Cambridge, ON. CA
    Posts
    111

    Default

    Quote Originally Posted by sw2x View Post
    I've been using the cheap gas lenses like what's available from welding city for about a yr now (off and on). I don't think I've ever used a standard collet to tig at all. But just today I got in my new CK130Flex and a Gas saver kit with the pyrex cup. I've fallen in love with these pyrex cups.. I CAN SEE THE ENTIRE PUDDLE! I've only layed one bead tonight after installing it, on some scrap aluminum, but I think it's the most consistent welding I've ever done. Seeing the puddle cool and the keyhole open up is key to knowing when to dip the rod again, with the clear cup I can see everything. I also noticed that the flow of argon is alot smoother through the gas saver kit than the standard gas lenses... Does everyone else with the pyrex gas saver kits notice the same thing over a standard gas lense?
    That comment made the descision for me. I was wondering what torch accessories to buy and it was a tossup between the gas lens and gas saver w/ pyrex cup. I always liked the idea of seeing the weld and have the benefit of gas economy. Some people have had opinions that the gas saver isn't worth it but I really like the idea. Guess if you just have to have it then the descision was made before you even thought about it.

    Where did you get the gas saver and how much, if you don't mind me asking?
    PowerArc 140ST
    Victor VPT-100FC

  15. #35

    Default

    Same here. I ended up ordering the standard-sized gas saver kit from arc-zone.com yesterday. It was $125 for a set with alumina and Pyrex nozzles in all the standard sizes. It comes with electrodes of different sizes as well.

    Sent from my PC36100 using Tapatalk 2
    Just a new guy that wants to make stuff.

    PowerPro 256

  16. Default

    Zank, would be nice if my welds looked like yours!!!
    Everlast PowerTig 200DX
    Miller 120 Mig

  17. #37

    Default

    Quote Originally Posted by greygizmo View Post
    Same here. I ended up ordering the standard-sized gas saver kit from arc-zone.com yesterday. It was $125 for a set with alumina and Pyrex nozzles in all the standard sizes. It comes with electrodes of different sizes as well.
    What electrodes are they shipping? Do not use the green tips (pure tungsten). Upload a picture when you get them. What torch was it for?
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  18. #38

    Default

    I bought my gas saver kit from weldfabulous.com

    CKCK130V FX CK130 Flex with valve torch $51.67
    CKD2GS116-P CK Gas Saver kit for 1/16 with Pyrex cup $21.97
    CKTAS332GS CK Tungsten Adapter w/screens for 3/32" $3.32
    CKTAS418GS CK Tungsten Adapter w/screens for 1/8" $3.32
    ------------
    Subtotal $80.28
    Shipping $9.20
    Total $89.48

    Torch did not include the hoses or the handle. Just the torch head itself
    Everlast PowerTIG 225LX
    Everlast Power IMIG 200

  19. #39

    Default

    Quote Originally Posted by willida View Post
    Zank, would be nice if my welds looked like yours!!!
    Thanks. Practice, practice, practice.

  20. #40
    Join Date
    Nov 2012
    Location
    Cambridge, ON. CA
    Posts
    111

    Default

    Quote Originally Posted by sw2x View Post
    I bought my gas saver kit from weldfabulous.com

    CKCK130V FX CK130 Flex with valve torch $51.67
    CKD2GS116-P CK Gas Saver kit for 1/16 with Pyrex cup $21.97
    CKTAS332GS CK Tungsten Adapter w/screens for 3/32" $3.32
    CKTAS418GS CK Tungsten Adapter w/screens for 1/8" $3.32
    ------------
    Subtotal $80.28
    Shipping $9.20
    Total $89.48

    Torch did not include the hoses or the handle. Just the torch head itself
    Looks like they changed their pricing for the gas saver kit. I can only find it for 25 and change now. If that's the price then that's what it is. Thanks for the details. I might try to find something closer to save on international shipping, if possible.
    PowerArc 140ST
    Victor VPT-100FC

Similar Threads

  1. Gas Lens Question
    By MCoupe in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 02-20-2014, 03:07 PM
  2. Simple Question from Newbie
    By tdkask in forum Everlast Plasma Cutters (PAC)
    Replies: 8
    Last Post: 09-21-2013, 07:41 PM
  3. Stupid newbie question
    By breakneckmot in forum General Welding Questions
    Replies: 9
    Last Post: 09-17-2013, 05:58 PM
  4. Newbie question
    By DaveO in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 03-14-2011, 08:02 PM
  5. Newbie 225LX pedal control question
    By robsthomson in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 02-17-2010, 01:25 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •